Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 30.0 microns | 1.18 mil | |
SABIC 218 Series Linear Low Density Polyethylene for Blown Film Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 218B Linear Low Density Polyethylene for Cast Film Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 518N Linear Low Density Polyethylene for Blown Film Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 6821N Linear Low Density Polyethylene for Blown Film Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi.. |
|||
Thickness | 30.0 - 150 microns | 1.18 - 5.91 mil | Recommended |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
Thickness | 30.0 - 150 microns | 1.18 - 5.91 mil | Recommended |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Thickness | 30.0 - 100 microns | 1.18 - 3.94 mil | Recommended |
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 30 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 30 µm) HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 3.5%; ASTM-252-78 |
Kinlead ML21 General Grade BOPP Matt Film (thickness: 30 µm) ML21 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. Both sides have corona treatment. It is specially designed for board lamin.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 30 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 30 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 30 µm) PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro.. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF260YZ Low density polyethylene LDF260YZ is a low density polyethylene resin for film extrusion. LDF260YZ has no slip and anti-block additives. LDF260YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF268GG Low density polyethylene LDF268GG is a low density polyethylene resin for film extrusion. LDF268GG has medium slip and anti-block additives. LDF268GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Thickness | 30.0 microns | 1.18 mil | Cured thickness on 175µm ITO coated polyester |
Gwent Electronic Materials C2061027P13 High Brightness Phosphor Ink (Blue/Green) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 30.0 microns | 1.18 mil | Cured thickness on 175µm ITO coated polyester |
Gwent Electronic Materials C2061027P15 High Brightness Phosphor Ink (Blue) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 30.0 microns | 1.18 mil | Cured thickness on 175µm ITO coated polyester |
Gwent Electronic Materials C2070209P5 High Brightness Phosphor Ink (Green) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF201FG Low density polyethylene LDF201FG is a low density polyethylene resin for film extrusion. LDF201FG has low slip and anti-block additives. LDF201FG meets the U.S. Food and Drug Administration (FDA) criteria for food contact .. |
|||
Thickness | 30.0 - 1100 microns | 1.18 - 43.3 mil | |
Schott D 263 Thin Borosilicate Glass D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang.. |
|||
Thickness | 30.0 - 1100 microns | 1.18 - 43.3 mil | wide range available |
Schott D 263® T eco Thin Borosilicate Optical Glass D 263® T eco thin glass is a clear borosilicate glass that has a high chemical resistance and is produced by the down-draw method. It is available in a variety of thicknesses ranging from 0.03 mm.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade DOW LDPE 609A resin is a fully formulated high strength clarity film resin for optical packaging applications, such as produce and bakery film. It contains medium levels of slip additive and low lev.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |