Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12 - 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
12 - 25 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 170 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 338 °F |
DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® 110 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 110 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a low thermoplasticity level.Applications: P.. |
|||
Melt Flow | 14 - 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 - 25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Kraton® G1643 M (SEBS) Linear Triblock Copolymer Description: Kraton G1643 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 20%. It is supplied from North America in the physical form ide.. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 150 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-781 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized... |
|||
Melt Flow | 15 - 25 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 - 25 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Shanghai Ofluorine Z-1 PVDF Injection Grade Description: Z-1 PVDF is a kind of granular homopolymer, which has low melt viscosity, Z-1 is more suitable for injection molding. Z-1 PVDF pellets as raw materials, the finished products has excell.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 900 Clear Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 930-05V0 White Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 980-05V0 Grey Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman SP980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 150 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-500 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 20 - 25 g/10 min @Temperature 230 °C |
20 - 25 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Melt Flow | 20 - 25 g/10 min @Temperature 230 °C |
20 - 25 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Melt Flow | 20 - 25 g/10 min @Temperature 230 °C |
20 - 25 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Melt Flow | 10 - 25 g/10 min @Load 8.70 kg, Temperature 210 °C |
10 - 25 g/10 min @Load 19.2 lb, Temperature 410 °F |
|
Lubrizol Estane® GP 58 DT Thermoplastic Polyurethane Type: Estane® GP 58DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ISO 1133 |
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5.. |
|||
Melt Flow | 15 - 25 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 - 25 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
E-Polymers EFLEX® M500 SEBS M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl.. |
|||
Melt Flow | 8.0 - 25 g/10 min @Load 3.80 kg, Temperature 232 °C |
8.0 - 25 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Melt Flow | 6.0 - 25 g/10 min @Load 12.5 kg, Temperature 232 °C |
6.0 - 25 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Melt Flow | 6.0 - 25 g/10 min @Load 12.5 kg, Temperature 232 °C |
6.0 - 25 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 741 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 190 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 374 °F |
DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperat.. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 150 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-560T TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 25 g/10 min @Load 12.5 kg, Temperature 232 °C |
8.0 - 25 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2850 PC Polyvinylidene Fluoride Spray Coating Powder Electrostatic sprayInformation provided by Arkema Inc. |