Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 190 °C |
55 g/10 min @Load 22.0 lb, Temperature 374 °F |
ISO 1133 |
Multibase TPSiV® 4000-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Reliance Industries Repol B550MN Polypropylene REPOL Polypropylene B550MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | ASTM D1238 |
ExxonMobil Santoprene® 912BA Thermoplastic Elastomer
(discontinued **) A hard, black, super high-flow thermoplastic olefin (TPO) in the thermoplastic elastomer (TPE) family. This grade of Vistaflex TPE is temperature-dependent and can be processed on conventional therm.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
M. Holland Company LL800 LLDPE
(discontinued **) Features: Fast Production Cycle, High Gloss, Low Temp. Impact Resistance, Low to No Odor, Low WarpageUses: Containers, Household Goods, Lids, Thin-walled PartsApprovals: FDA 21 CFR 177.1520(c) 3.2a .. |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 300 °C |
55 g/10 min @Load 11.0 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 50/TF/15/NAT Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | ASTM D1238 |
Hyosung Topilene J945 PP J945 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos R55C-00 Clarified Polypropylene Copolymer Grade R55C-00 is a high melt flow rate clarified and antistatic random polypropylene copolymer. It is designed for high speed injection molding of thin walled parts requiring very good mold filling .. |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 260 °C |
55 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 260 °C |
55 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® B 3217 XF 000000 PBT, 16% Glass Fiber PBT, 16% glass fibers, injection molding, improved flowability, impact modified |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 275 °C |
55 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Gromax BFG30-BN00B2 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 266 °C |
55 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 250 °C |
55 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HJ320MO Polypropylene HJ320MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. This grade is .. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 g/10 min @Temperature 230 °C |
55 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for inje.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPH 11012 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 11012 is a nucleated controlled-rheology antistatic homopolymer with a high melt flow index of 55 g/10 min.Polypropylene PPH 11012 is characterized by high fluidity for high speed .. |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | Cond. E; ASTM D1238 |
DuPont Conpol™ 20S2 Ethylene-Methacrylic Acid Additive Resin Conpol™ additive resins, supplied in pellet form, are designed to modify the surface properties of films or coatings of Surlyn® ionomer resins and Nucrel® acid copolymer resins. They are concentr.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D 1238 |
Cossa Polimeri ESTAPROP HK 4000 CH-HT Polypropylene Copolymer Polypropylene copolymer, high fluidityInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg |
55 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8. |
Dow LDPE 959I Low Density Polyethylene DOW LDPE 959I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility with low warpage for lids. This resin has good processability over a wi.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® W 77 AV Polypropylene Homopolymer CAPILENE® W 77 AV is a very high melt flow rate polypropylene homopolymer for injection molding with antistatic and nucleating additives. It offers a good balance of stiffness and flow, high de-mol.. |
|||
Melt Flow | 55 - 65 g/10 min | 55 - 65 g/10 min | ISO 1133 |
Beijing Ranger Chem BLUESTAR® 1084 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |