Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 912BA Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 912BA Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A hard, black, super high-flow thermoplastic olefin (TPO) in the thermoplastic elastomer (TPE) family. This grade of Vistaflex TPE is temperature-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.Recommended for applications requiring good UV resistance, impact resistance, paintability, high flow and medium modulus. Recommended for applications requiring superior part surface appearance.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Melt Flow 55 g/10 min
55 g/10 min
ASTM D1238
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 118
Color Natural Color
Form Pellets
Users viewing this material also viewed the following: