Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 8502-SR BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products G20P100-01UV 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Rigid exterior componentsHousingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers 779 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
KKPC Kuhmo GP 125BL Extrusion Molding GPPS Key features: PSP Common Uses: Sheeting, instant noodle cups.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability o.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 266 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Luriblend® ABS SL2 Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 2.20 kg |
4.5 g/10 min @Load 4.86 lb |
ASTM D1238 |
Sumitomo Chemical ESPOLEX® UT412A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSI 3441 High Heat Resistance Impact Polystyrene Total Petrochemicals Polystyrene 3441 is a high heat resistance, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional st.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total PSI 8350 High Impact Polystyrene 8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis CA7230 Low Density Polyethylene CA7230 is a low-density polyethylene for extrusion coating. CA7230 contains no additives. Applications: Extrusion coating of high volume production of boards and papers. Coating of various plasti.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
ExxonMobil Exceed™ 4518PA Premium Cast Film Resin Exceed 4518PA resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 4518PA resin have outstanding tensile properties and impact and puncture toughness.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HD 6704.18 High Density Polyethylene Copolymer Resin Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
condition E; ASTM D1238 |
DuPont™ Surlyn® 9150 Ionomer Resin, Zinc Surlyn® 9150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The high MAA content and mi.. |
|||
Melt Flow | 4.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GM7746C HDPE Blow Molding Polyethylene GM7746C is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tenac.. |
|||
Melt Flow | 4.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GM7746CA HDPE Blow Molding Polyethylene GM7746CA is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tena.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between goo.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
Asahi Kasei Thermylene® P6-40FG-0700 40% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Melt Flow | 4.5 g/10 min @Temperature 190 °C |
4.5 g/10 min @Temperature 374 °F |
High Load; ISO 1133 |
Total ESD 201 B HDPE blow molding FINATHENE® ESD 201 B is a black conductive compound manufactured from high performance Finathene high density polyethylene. The use of this HDPE compound gives outstanding compatibility to (semi) h.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Resirene Resirene® 7600 Super High Impact Polystyrene Features:Medium FlowSuper High ImpactEasy ProcessingHigh ProductivityFDA Rating: 21 CFR 177.1640Applications:InjectionToysCompounds and Master BatchPrintersComputersRemote ControlsInformation provid.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 343 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 343 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Melt Flow | 4.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min |
Polimeri Europa SINKRAL PD C823 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, exhibiting very high impact resistance, even at low temperatures. Applic.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem HD7255LS-L HDPE Injection Molding Polyethylene HD7255LS-L is a high-density polyethylene developed for injection molding. It has good tenacity and impact properties combined with good stiffness. It presents a ratio between melt flow and density .. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Luriblend® ABS X MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po.. |