Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.908 g/cc
0.0328 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0096 cm/cm
0.0096 in/in
ASTM D955
Melt Flow 4.5 g/10 min
4.5 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
10 sec; ASTM D-2240
Tensile Strength, Ultimate 8.90 MPa
1290 psi
ASTM D412
Elongation at Break 490.8 %
490.8 %
ASTM D412
Flexural Modulus 0.0780 GPa
11.3 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 76.0 kN/m
434 pli
ASTM D624