Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polyplastic TechnoTep B® 60 A Thermoplastic Elastomer, Mineral Filled Medium mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® GM 20 Low Density Polyethylene - Coating Grade Riblene GM 20 is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 20 is suitable for coating applications where a low neck-in is required. Moreover, for its rh.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP550K Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP550K is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP550K is a homopolymer suitable for rope, tape, yarn, monofilament.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips Sumika Marlex® CHP-010 Thermoplastic Polyolefin
(discontinued **) Applications: Soft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Melt Flow | 3.5 g/10 min | 3.5 g/10 min | ASTM D1238 |
ExxonMobil LL 1235x70 Cast Film Resin
(discontinued **) LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova 50 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High strength crystal polystyrene, High heat crystal polystyrene, Custom colorsApplications: Injection molding or extrusion, Designed for applications requiring strength and high heat resistance whe.. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® TR-0338-UIG Hexene MDPE Rotational Molding Resin Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, .. |
|||
Melt Flow | 3.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Centrex® 601 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionInformation.. |
|||
Melt Flow | 3.5 g/10 min @Load 1.00 kg, Temperature 235 °C |
3.5 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegisâ„¢ H85QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H85QP is a lubricated, medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 a.. |
|||
Melt Flow | 3.5 g/10 min | 3.5 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (0.5 mil Film) ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |
|||
Melt Flow | 3.5 - 6.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 - 6.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Kraton® D1163 J (SIS) Linear Block Copolymer Description: Kraton D1163 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t.. |
|||
Melt Flow | 3.5 g/10 min | 3.5 g/10 min | ISO 1133 |
Lucite International Diakon® TD510 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 25SPI GPPS High strength, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Sup.. |
|||
Melt Flow | 3.5 g/10 min @Load 10.0 kg, Temperature 230 °C |
3.5 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Statiblend® POM CO Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeature: ConductiveTPCI# 9962114Information provided by TP Composites, Inc. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HF-0660IW ABS, Unreinforced WNP high flow ABS materialInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® NH-0700FX ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HF-0660IW ABS, Unreinforced WNP high flow ABS materialInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® VE-0812 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Appeel® LSR20D752 Lidding Sealant Resin Appeel® LSR20D752 is a modified ethylene acrylate copolymer designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Melt Flow | 3.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Polyram RamTough RZ300G6 Polycarbonate, 30% Glass Fiber 30% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSC 529 Polystyrene Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil PP2252E1 Homopolymer Product Description: Medium melt flow rate homopolymer designed for high speed extrusion of woven fabrics exhibiting low water carry over.Availability: North America Features:Balanced Stiffness/To.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 503 Injection Molding Polypropylene Description: H 503 is a low melt flow rate additivated homopolyme used for general purposes. It is designed for injection molding, raffia extrusion, bioriented film and general extrusion. This produ.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem H 503 Raffia Extrusion & Fiber Extrusion Polypropylene Homopolymer ApplicationsRaffia Extrusion: Industrial bags; Flexible containers; Curtains and covers to aviary and agriculture.Fiber Extrusion: Monofilament for ropes; Fishing nets; Cables and ropes for boats; .. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
D-1238 |
Bapolene® 4042 Polypropylene, Fiber/Filament Grade Bapolene PP4042 is a fiber extrusion resin with excellent thermal and mechanical properties. This product meets FDA standards for food contact applications.Applications: Rope and twine, fibrillated.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 501 HC Injection Molding Polypropylene Description: H 501HC is a low melt flow rate homopolymer, designed for very high stifness aplications with good processability. This product exhibit excellent chemical resistance and barrier propert.. |