Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem H 503 Raffia Extrusion & Fiber Extrusion Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem H 503 Raffia Extrusion & Fiber Extrusion Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsRaffia Extrusion: Industrial bags; Flexible containers; Curtains and covers to aviary and agriculture.Fiber Extrusion: Monofilament for ropes; Fishing nets; Cables and ropes for boats; Bristles for toothbrushes and brooms.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D792
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus, 1% Secant 1400 MPa
203000 psi
ASTM D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
208 °F
ASTM D648
Descriptive Properties Value Comments
Molecular Weight Distribution Normal
Users viewing this material also viewed the following: