Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 29 g/10 min | 29 g/10 min | I<sub>21</sub>; ASTM D238 |
Petromont 1000 High Density Polyethylene Resin Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to .. |
|||
Melt Flow | 29 g/10 min | 29 g/10 min | I<sub>21</sub>; ASTM D238 |
Petromont 1002 High Density Polyethylene Resin Petromont HDPE 1002 is a blow moulding high-density polyethylene copolymer resin produced using the UNIPOL® Process. This multi-purpose resin can be used on intermittent and continuous extrusion bl.. |
|||
Melt Flow | 29 g/10 min | 29 g/10 min | ISO 1133 |
Solvay Engineered Polymers SEQUEL® 1402 TPO
(discontinued **) Description: SEQUEL® 1402 engineered polyolefin material is designed for large automotive exterior applications that require high melt flow, excellent paintability, and processability. Applications.. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 260 °C |
29 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific) Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives. |
|||
Melt Flow | 29 g/10 min @Load 5.00 kg, Temperature 190 °C |
29 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 58 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e.. |
|||
Melt Flow | 29 g/10 min @Load 1.20 kg, Temperature 300 °C |
29 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BFL2000B PC (Asia Pacific) Lexan BFL2000B resin is a Br- & Cl-free FR polycarbonate resin featuring high flow with balanced impact. It is available only in dark colors. |
|||
Melt Flow | 29 g/10 min @Load 1.20 kg, Temperature 224 °C |
29 g/10 min @Load 2.65 lb, Temperature 435 °F |
|
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta.. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 330 °C |
29 g/10 min @Load 4.76 lb, Temperature 626 °F |
cm³/10 min. |
Covestro Apec® 1605 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation pr.. |
|||
Melt Flow | 29 g/10 min | 29 g/10 min | ISO 1133 |
LyondellBasell SEQUEL® 1480 Engineered Polyolefin Description: SEQUEL® 1480 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paintability,.. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 230 °C |
29 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Integrateâ„¢ NP507030 Functionalized Polyolefin INTEGRATE products are chemically modified polyolefins used to combine dissimilar materials for a variety of applications including molding articles, flexible materials and fiber technology or to pr.. |
|||
Melt Flow | 29 g/10 min @Load 5.00 kg, Temperature 200 °C |
29 g/10 min @Load 10.8 lb, Temperature 392 °F |
|
Kraton® D1117 P (SIS) Linear Block Copolymer Description:Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: K.. |
|||
Melt Flow | 29 g/10 min @Load 5.00 kg, Temperature 200 °C |
29 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Kraton® D1117 P (SIS) Linear Triblock Copolymer Description: Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: .. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 230 °C |
29 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Kuraray SEPTON® PM1 Polypropylene Modified Plastic Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 260 °C |
29 g/10 min @Load 4.76 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® KL 1-7265 000000 PBT, 15% Glass Fiber PBT, 15% glass fibers, injection molding |
|||
Melt Flow | 29 g/10 min @Load 5.00 kg, Temperature 260 °C |
29 g/10 min @Load 11.0 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Melt Flow | 29 g/10 min @Load 10.0 kg, Temperature 220 °C |
29 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® LX-0951 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 29 g/10 min @Load 10.0 kg, Temperature 220 °C |
29 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® LX-0951 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 230 °C |
29 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 230 °C |
29 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 230 °C |
29 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 230 °C |
29 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 230 °C |
29 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Melt Flow | 29 g/10 min @Load 5.00 kg, Temperature 260 °C |
29 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Covestro Makroblend® DP UT5005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding gradeMakroblend DP UT5005* provides an outstanding balance of low-temperature impact strength and flowability beside e.. |
|||
Melt Flow | 29 g/10 min @Load 5.00 kg, Temperature 260 °C |
29 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow.. |
|||
Melt Flow | 29 g/10 min @Load 5.00 kg, Temperature 265 °C |
29 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
Diamond Polymers ABSPC 7801 ABS/PC Injection Molding Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 190 °C |
29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem IC32 LLDPE Injection Molding Polyethylene Copolymer IC32 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding. It offers good fluidity, excellent flexibility and tenac.. |
|||
Melt Flow | 29 g/10 min @Load 10.0 kg, Temperature 360 °C |
29 g/10 min @Load 22.0 lb, Temperature 680 °F |
ISO 1133 |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Melt Flow | 29 g/10 min @Load 2.16 kg, Temperature 230 °C |
29 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |