Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 14 g/10 min | 14 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 4012 X Platinum Polypropylene Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products M25P251-01A 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsInternal I/P componentsFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 230 °C |
14 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 51 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow INSPIRE™ DT701-14 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 200 °C |
14 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Data |
Americas Styrenics Styron® 615APR Polystyrene
(discontinued **) STYRON® 615 APR is a general purpose easy flow resin typically used for medical, pharmaceutical and thin-walled parts. It is an excellent resin for blending with K-Resin (K-Resin is a trademark of .. |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 925 PC Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa.. |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
Lehmann & Voss LUVOCOM® 1200-7116 ABS, with carbon fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 290 °C |
14 g/10 min @Load 22.0 lb, Temperature 554 °F |
ASTM D1238 |
M. Holland Company AB103LG ABS Acrylonitrile Butadiene Styrene Medium flowMedium impact resistanceGood stiffnessInformation provided by M. Holland |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 200 °C |
14 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D1173 B (SIBS) Linear Triblock Copolymer Description: Kraton D1173 B is a clear, linear triblock copolymer based on styrene, butadiene and isoprene with a polystyrene content of 18%. It is supplied from Brazil in the form: Kraton D1173 BT .. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 280 °C |
14 g/10 min @Load 11.0 lb, Temperature 536 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 210 °C |
14 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP821U PPE-TPE (Asia Pacific) UV stabilized, halogen free Flexible Noryl injection molding grade for overmolding applications such as plugs, strain relief's, and connectors. Good color stability after UV weathering per ASTM D445.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 250 °C |
14 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 250 °C |
14 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133; ASTM D1238 |
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar.. |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samyang Trirex® 3022PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022PJ is a general use grade.Information provided by Samyang. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 260 °C |
14 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP High modulus/impact/heat PPE+PP |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 260 °C |
14 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PPX PPX7115F PPE+PP High modulus/impact/heat PPE+PP. Compliant with US FDA food contact regulations for temperatures of use of room temperature and below. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 200 °C |
14 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total PS CPDS 807 Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 807 is a high impact flame retardant polystyrene for use in HGW applications. PS CPDS 807 can be supplied in both natural and colored forms.Main Characteristics:DBD.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3251V Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3251V is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3251V conta.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 190 °C |
14 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
ELASTO UK Mediprene™ 660420M TPE, Medical Applications, 42A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
Melt Flow | 14 g/10 min @Load 1.00 kg, Temperature 235 °C |
14 g/10 min @Load 2.20 lb, Temperature 455 °F |
|
Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 130 HD POM Copolymer unreinforced, improved fuel resistance POMInformation provided by BARLOG plastics GmbH. |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Melt Flow | 14 g/10 min | 14 g/10 min | ASTM D1238 |
Asahi Kasei Thermofil P-40TC-5100 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Melt Flow | 14 g/10 min | 14 g/10 min | ASTM D1238 |
Aaron Industries AAROLENE® AVPS HIPS 100-3 MELT 14 Virgin HIPS Resin A virgin, high impact polystyrene, natural in color, specifically designed for injection molding applications. |
|||
Melt Flow | 14 g/10 min | 14 g/10 min | ISO 1133 |
Addiplast Addilene H 442 M30 Polypropylene Homopolymer High heat resistance, detergent stabilizedInformation provided by Addiplast. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 300 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3000 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |