Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Reliance Industries Repol R019MZ Polypropylene REPOL Polypropylene R019MZ is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 250 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND HI 40 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified blend PBT+PC blend with very good impact behaviour, ductility even at low temperatures, resistant to solvents, good dimensional stabilit.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-134 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills 43S2A Polypropylene Random Copolymer Features: Good clarity.Applications: Film extrusion and blow moldingInformation Provided by Flint Hills Resources |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills P5L2K-055 Polypropylene Random Copolymer Features: Excellent clarity. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: extrusion blow molding, injection blow molding, stretch blow moldin.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos R01C-01 Polypropylene Random Copolymer This is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding. Applications that require good see-through clarity combined with good heat resistance .. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE3-0200RX Biocompatible LDPE A biocompatible Low Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE3-0205ARX Biocompatible, Antimicrobial LDPE A biocompatible Low Density Polyethylene for healthcare applications containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Color Compo.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills P5M2Z-012 Polypropylene Random Copolymer Features: Good contact clarity. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: film and blow moldingInformation Provided by Flint Hills Resources |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex ELEXAR® EL 8712 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Bormed™ RB801CF Polypropylene Random Copolymer Bormed™ RB801CF is a random copolymer. Applications: Bormed™ RB801CF is intended for packaging for medical devices, pouches, and packaging for pharmaceutical products. Additives: Bormed™ RB801C.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications Bormed RB845MO is a random copolymer for blow molding with very good transparency and high contact clarity, very good gloss and surface finish. Bottles in sizes up to 2 quarts molded from Bormed RB.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont 20 Series 2010 Specialty Polyethylene Resin DuPont 2010 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding fl.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont 20 Series 20-6064 Specialty Polyethylene Resin DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RB206MO Polypropylene Random Copolymer RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also .. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a.. |
|||
Melt Flow | 1.9 g/10 min @Temperature 230 °C |
1.9 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow 6D20 Polypropylene Resin DOW 6D20 is intended for use in film and extrusion blow molding processes. It is especially suited for multilayered, barrier bottles.Information provided by DowDow Announced Sale of Global Polyprop.. |
|||
Melt Flow | 1.9 g/10 min @Temperature 230 °C |
1.9 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow INSPIRE™ D560.00 Developmental Performance Polymer D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended f.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg |
1.9 g/10 min @Load 4.76 lb |
|
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg |
1.9 g/10 min @Load 4.76 lb |
|
Dow LDPE 503A Low Density Polyethylene, Liner Film Grade DOW LDPE 503A resin is used for liner film and other packaging applications that require optical clarity. It contains medium levels of slip additive and low levels of antiblock additive. It complies.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem PB682 Blow Molding Low Density Polyethylene Blow molding; Injection blow molding; Medium resistance mechanical film; Expanded PE blankets.Information provided by Braskem. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® E 65 F Polypropylene Homopolymer Description: CAPILENE® E 65 F is a polypropylene homopolymer designed for the production of biaxially oriented polypropylene films (BOPP). It exhibits good processability, easy film stretchabilit.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene Product CharacteristicsGood impact resistanceConsistent colorabilityEasy processingFood Contact CompliantUL Classification 94HBTypical ApplicationsExtruded SheetSmall AppliancesRefrigeration Accesso.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | Condition G |
Ineos Nova 1220 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
M. Holland Company MAGMA® LM213-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg |
1.9 g/10 min @Load 4.76 lb |
|
Dow LDPE 535I Low Density Polyethylene, Liner Grade DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for.. |