Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® PF-Y821-CP Butene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Sclair® FP019-D Octene Copolymer LLDPE Film Resin FP019-D is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Slip, Antiblock, Polymer Process AidApplications: Hig.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin
(discontinued **) Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 5658 LDPE Shrink and Bundling Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Abrasion and Tear Resistance, Good Sealing Properties, No Slip, Medium Antiblock, Easy OpenabilityApplications:Shrink Wrap, Bundlin.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 5758 LDPE High Clarity, High Impact Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, Medium Antiblock, Moderately High Coefficient of Friction, Easy Openability of BagsApplications:Case Shr.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
Huntsman PE 1008 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | Exxon Method |
ExxonMobil Iotek® 8000 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.61 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 5.75 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC ST308 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Hifaxâ„¢ CA10GC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA10GC fractional melt flow, 100 MPa flexural modulus, precolored, UV-stabilized, reactor grade, extrudable thermoplastic elastomeric olefin (TEO) resin combines good proces.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Hifaxâ„¢ CA260GC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA260GC White fractional melt flow, 40 MPa flexural modulus, UV-stabilized, precolored thermoplastic elastomeric olefin (TEO) resin has an excellent balance of flexibility,.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | ISO 1133 |
Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Melt Flow | 0.80 - 2.0 g/10 min | 0.80 - 2.0 g/10 min | |
Shandong Dongyue Shenzhou New Material Co DS602 Perfluorinated Ethylene-Propylene Copolymer Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | ISO 1133 |
Total FE 8004 LDPE blown film Radical polyethylene made by high pressure autoclave process. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former F.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 5754 LDPE High Clarity, High Impact Film Resin for General Purpose Packaging Resin Type: HomopolymerCharacteristics: Excellent Impact Strength, High Clarity, Medium Slip, Medium Antiblock, Low Coefficient of Friction, Good OpenabilityApplications:Heavy Produce Bags, Frozen F.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 3201.69 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers NPP25-0116 Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th.. |
|||
Melt Flow | 0.80 - 1.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Breplast Bretene LD BT Thermoplastic Composite, 50% LD + 50% PP Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount. The minimum biobas.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | Exxon Method |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH008 Polypropylene, Homopolymer, Netting COPYLENE™ CH008 is a fractional melt flow polypropylene homopolymer resin available in pellet form. Applications: Raffia/Tapes/Strapping; Anti-Corrosion Coating; Geotextile & Agriculture; Nets. Rep.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
E-Polymers EFLEX® I1020 Ionomer I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnes.. |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC SF316 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Additives- Medium slip agent, Medium antiblocking agentApplications: Agricultural & i.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11H1 LLDPE Film Resin
(discontinued **) Low gel, Excellent heat sealability, Easy processability, High toughness and strengthApplications: Heavy duty sack, High strength packagingAdditives: Process stabilizer, Polymer process aid, Antiblo.. |