Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12 - 16 g/10 min | 12 - 16 g/10 min | ASTM D1238 |
S&E Specialty Polymers GPP™ 1005M-EXLT PP Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers |
|||
Melt Flow | 4.0 - 16 g/10 min | 4.0 - 16 g/10 min | ASTM D1238 |
Polymer Resources ABS-FR1 ABS, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 14 - 16 g/10 min | 14 - 16 g/10 min | ASTM D1238 |
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Melt Flow | 12 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Kingfa PC-S609 Toughened PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Melt Flow | 10 - 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
10 - 16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
GRECO ISOPAK 625 Polycarbonate/ABS Alloy General purpose polycarbonate/ABS alloy; good impact and dimensional stabilityInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Melt Flow | 12 - 16 g/10 min | 12 - 16 g/10 min | Cond L; ASTM D1238 |
Washington Penn PPH4CF2.5 Polypropylene, 25% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: High flow for thin wall parts requiring long-flow. Outdoor furniture.Data provided by Washington Penn Plastic Co., Inc. |
|||
Melt Flow | 12 - 16 g/10 min | 12 - 16 g/10 min | Cond L; ASTM D1238 |
Washington Penn PPH5CF5 Polypropylene, 50% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: Commonly used as a concentrate. High flow for thin wall parts requiring long-flow. Toys, small appliances, outdoor furniture.Data provided by W.. |
|||
Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 5.00 kg, Temperature 372 °C |
8.0 - 16 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Melt Flow | 12 - 16 g/10 min | 12 - 16 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPPC 2010 CW Polypropylene, Calcium Filled Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro.. |
|||
Melt Flow | 10 - 16 g/10 min | 10 - 16 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Melt Flow | 14 - 16 g/10 min | 14 - 16 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 6421 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 12.1 - 16 g/10 min | 12.1 - 16 g/10 min | D |
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff.. |
|||
Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
DuPont Elvaloy® HP663 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
(discontinued **) Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |