Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC PP 413MNK45 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic package & nucleating agent and is especially developed for producing.. |
|||
Melt Flow | 70 - 85 g/10 min @Load 2.16 kg, Temperature 210 °C |
70 - 85 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6251D Fiber Grade PLA NatureWorks® PLA polymer 6251D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6251D is designed for spunbond products using conv.. |
|||
Melt Flow | 70 g/10 min | 70 g/10 min | ExxonMobil Method |
ExxonMobil LD 509.48 Compounding Resin
(discontinued **) LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 70 g/10 min | 70 g/10 min | ASTM D1238 |
LyondellBasell Microthene® G MN70100 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melt Flow | 70 g/10 min @Load 1.20 kg, Temperature 300 °C |
70 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LG Chemical Lupoy 1080-70 Polycarbonate Resin Description: LUPOY PC 1080-70 resin is designed for optical media discs applications. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Ch.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 250 °C |
70 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D 1238 |
SABIC Innovative Plastics Valox® 295 PBT Unreinforced PBTThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Sanyo J-STAT 3180 Antistatic Additive Information provided by Tomen America, a US distributor of Pelestat. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Bormod™ BJ368MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tec.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate DescriptionPOLYBATCH® AC-20531L is a UV absorber concentrate containing 20% active additive based in low density polyethylene. POLYBATCH® AC-20531L is designed for use in polyethylene blown and c.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RJ470MO Polypropylene, Transparent Random Copolymer RJ470MO is a specially modified highly-transparent polypropylene random copolymer with very high melt flow rate and is designed for high-speed injection molding and contains nucleating and demolding.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate DescriptionPOLYBATCH® AC-20531L is a UV absorber concentrate containing 20% active additive based in low density polyethylene. POLYBATCH® AC-20531L is designed for use in polyethylene blown and c.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1700 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade for easy flow injection molding of flexible parts, powder production for grindin.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 11712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 11712 is a nucleated controlled-rheology heterophasic copolymer. PPC 11712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate DescriptionPOLYBATCH® AC-20531L is a UV absorber concentrate containing 20% active additive based in low density polyethylene. POLYBATCH® AC-20531L is designed for use in polyethylene blown and c.. |
|||
Melt Flow | 70 - 130 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 - 130 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
DuPont Elvaloy® HP771 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate DescriptionPOLYBATCH® AC-20531L is a UV absorber concentrate containing 20% active additive based in low density polyethylene. POLYBATCH® AC-20531L is designed for use in polyethylene blown and c.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate DescriptionPOLYBATCH® AC-20531L is a UV absorber concentrate containing 20% active additive based in low density polyethylene. POLYBATCH® AC-20531L is designed for use in polyethylene blown and c.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 160 °C |
70 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 160 °C |
70 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications) GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent r.. |
|||
Melt Flow | 70 g/10 min | 70 g/10 min | ASTM D1238 |
ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade) Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East.. |
|||
Melt Flow | 70 g/10 min @Load 10.0 kg, Temperature 220 °C |
70 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polylac® PA-756S ABS - High Flow Super high flow, medium impact |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI4700P2 Impact Copolymer Polypropylene Description: Very high flexural modulus.Applications: Suggested uses include compounding, automotive interior trim, intricately designed parts, thinwalled parts, dairy containers, building and const.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
"E"; ASTM D1238 |
Aaron Industries AAROPRENE® ATPR 1000 80A Elastomeric Compound AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified. |
|||
Melt Flow | 70 g/10 min @Load 5.00 kg, Temperature 275 °C |
70 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate DescriptionPOLYBATCH® AC-20531L is a UV absorber concentrate containing 20% active additive based in low density polyethylene. POLYBATCH® AC-20531L is designed for use in polyethylene blown and c.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 6221 CUV A Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 6221 CUV A VY Dk Pewter TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 235 °C |
70 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238R |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |