Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers PC-1006 Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers PC-1006 L Description: Colors and Natural Polycarbonate with UVInformation provided by Network Polymers Inc. |
|||
Melt Flow | 6.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
without Catalyst MB addition; Internal Method |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 0.5 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
Formosa Plastics Formolene® LH5206 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, lidsFormolene LH5206 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as specified in 2.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.06 kg, Temperature 343 °C |
6.5 g/10 min @Load 4.54 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
(Unverified Data**) Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
LyondellBasell Alathon® M5363 High Density Polyethylene ApplicationsALATHON L 4912 is a high molecular weight, high density copolymer with a broad molecular weight distribution. This resin provides excellent stiffness and a good balance of film properti.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA336149 Low Density Polyethylene ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
LyondellBasell Plexar® PX5125 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE ApplicationsPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copo.. |
|||
Melt Flow | 6.5 - 10.5 g/10 min | 6.5 - 10.5 g/10 min | ASTM D1238 |
Kolon KOCETAL® UR304 Toughened Grade Acetal Resin TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon. |
|||
Melt Flow | 6.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
6.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Ineos ABS Lustran® SAN GF20 Glass Fiber Reinforced |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
KKPC Kuhmo HI 450PG High Gloss HIPS Common Uses: Monitor swivels, washers.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resistance and heat-resistance.Data pr.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 343 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU), Glass Fiber Udel® GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Melt Flow | 6.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
6.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 9035 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 6.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
6.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Melt Flow | 6.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
6.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ISO 1133 |
Styron TYRILâ„¢ 875 SAN Resin Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White P8555 SD Concentrate Based In Homopolymer Polypropylene DescriptionPOLYBATCH® P8555 SD is a white masterbatch containing 50% TiO2 based in homopolymer polypropylene. This product offers excellent dispersion and a very low moisture content which permits.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White P8555 SD Concentrate Based In Homopolymer Polypropylene DescriptionPOLYBATCH® P8555 SD is a white masterbatch containing 50% TiO2 based in homopolymer polypropylene. This product offers excellent dispersion and a very low moisture content which permits.. |
|||
Melt Flow | 6.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
6.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Total PSC 1450N High Heat Resistance Polystyrene 1450N is a high heat resistance, easy flowing crystal polystyrene for the production of thick insulation board. The low viscosity of this grade makes it particularly suitable for the production of .. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ ED213AE TPO Compound Daplen ED213AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen ED213AE is a material with excellent impact/ stiffness ratio. Thanks to its low.. |
|||
Melt Flow | 6.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Melt Flow | 6.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content |
|||
Melt Flow | 6.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
6.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 7535 Injection Molding Grade, Very High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 6.5 g/10 min @Load 10.0 kg, Temperature 230 °C |
6.5 g/10 min @Load 22.0 lb, Temperature 446 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 908 EL POM Copolymer unreinforced, impact modified POM-IInformation provided by BARLOG plastics GmbH. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EMAC® SP2403 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2403 is a 24% EMA copolymer designed for extrusion coating, tie-layers, compounding, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Melt Flow | 6.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Amco Amalloy® B9674 Polymer Alloy Amco Amalloy B9674 is a clear performance copolymer with exceptional clarity and toughness.Good melt flow, and impact strength.Information provided by Amco Plastic Materials. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | Condition G |
Ineos Nova 4501 Medium Impact Polystyrene
(discontinued **) Good toughnessApplications: Light louvers, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provide.. |