Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 0405 Polypropylene Features: Impact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND HI 20 PBT+PC, Impact Grade
(discontinued **) PBT elastomer modified with good impact behaviour, good stiffness, resistant to solvents. Main application fields: automotive industryUnfilled. Suitable for Injection Molding. Supplied as pellets.. |
|||
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | ASTM D1238 |
ExxonMobil LLP8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |
|||
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | ASTM D1238-62T |
Chevron Phillips 4518 LDPE Extrusion Coating Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Processability, Improved Drawdown, Good MVTR, Good Heat Seal, Kosher ApprovedApplications:Liquid Packaging, Cup Stock, Folding CartonData provided b.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman E6837-539A Polyethylene
(discontinued **) PolyethyleneE6837-539A is used in various injection molding applications including closures for containers or extrusion coating for high stiffness. It has good processability. This product may be us.. |
|||
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |
|||
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 400 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 752 °F |
ASTM D1238 |
Solvay Specialty Polymers Supradel® HTS-2630 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2630 is a 30% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance .. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
MBA Polymers PP 2126 Post-consumer recycled general purpose polypropylene impact copolymer Available in standard black.Information provided by MBA Polymers. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical LUPOY MP5000AM PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ISO 1133 |
LyondellBasell Adsylâ„¢ 3 C 30 F HP Polypropylene Copolymer Description: Adsylâ„¢ 3 C 30 F HP is a new alpha olefin modified polypropylene copolymer especially designed for Bopp Film technology. The grade is formulated with a general purpose stabilization.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ISO 1133 |
LyondellBasell Adsylâ„¢ 5 C 30 F Polyolefin Description: Adsylâ„¢ 5 C 30 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity a.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ISO 1133 |
LyondellBasell Adsylâ„¢ 5 C 39 F Polyolefin Description: Adsylâ„¢ 5 C 39 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity an.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Adsylâ„¢ 5C37F Thermoplastic Olefin Resin Primary Processing Method: Film extrusionKey Features: thermoplastic olefin resins for film extrusion, good clarity and gloss, good moisture barrier properties, very low seal initiation temperature,.. |
|||
Melt Flow | 5.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2410R PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 5.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5211R PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Melt Flow | 5.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5211R PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Supreme Petrochem SP 243 Toughened Polystyrene CharacteristicsGood flexibility Good clarity High stiffnessProcessing Extrusion ThermoformingApplications Clear thermoformed containers Oriented PS films LidsMaterial Status: Commercial : ActiveA.. |
|||
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Supreme Petrochem SP 263 Toughened Polystyrene CharacteristicsGood flexibility Easy flow Good stiffnessProcessing Injection moldingApplications Transparent hangers Material Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640Informatio.. |
|||
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Supreme Petrochem SP6415 High Gloss High Impact Polystyrene Characteristics Very good gloss with the retention of ESCR properties Good toughness Also available in various color shades Processing Injection moldingApplications Refrigerator end caps Refriger.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 330 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 626 °F |
|
Covestro Apec® HT KU 1-9363 High-Heat Polycarbonate, UV-Stabilized Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ FL 00623 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00623 is a good coextrusion partner in extrusion coating, blown and cast film. Excellent sealing material with a very low seal initiation temperature. Availability: Africa & .. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle.. |
|||
Melt Flow | 5.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polyrex® PH-60 Polystyrene - High Impact Medium impact |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg |
5.5 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 7.5. |
Dow DOWLEX™ 3010 Linear Low Density Polyethylene DOWLEX® 3010 Polyethylene resin is a polyethylene polymer designed to offer high performance properties such as excellent environmental stress crack resistance, tear strength, abrasion resistance, .. |
|||
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | ASTM D1238 |
Engineered Plastics EP Alloy 510G PC/ABS Alloy Black. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Proper.. |
|||
Melt Flow | 5.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Amco Amalloy® B1025 Polymer Alloy Amco Amalloy B1025 is a clear performance copolymer with exceptional clarity and toughness.Clear, medium melt-flow.Information provided by Amco Plastic Materials. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |