Description: Adsyl™ 3 C 30 F HP is a new alpha olefin modified polypropylene copolymer especially designed for Bopp Film technology. The grade is formulated with a general purpose stabilization package and does not contain any slip nor antiblock agents. Adsyl™ 3 C 30 F HP is specifically studied for metallized skin layers to increase metal adhesion and enhance barrier properties on metallized film. Adsyl™ 3 C 30 F HP features a Seal-Initiation Temperature (SIT) of 112°C measured on bi-oriented film of 30 µm. With a Melting Point at 140°C, this grade exhibits an exceptionally broad processability range of temperature. The composition of the product complies with FDA norms and with regulations in force in major European concerning food contact applications. Uses: bi-oriented filmInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ISO 1133
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 112 °C

@Thickness 1.20 mm
234 °F

@Thickness 0.0472 in
Thermal Properties Metric English Comments
Melting Point 140 °C
284 °F
MTM 15902