Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 37 g/10 min @Load 2.16 kg, Temperature 230 °C |
37 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 25-3701 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Melt Flow | 37 g/10 min @Load 5.00 kg, Temperature 260 °C |
37 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance. |
|||
Melt Flow | 37 g/10 min @Load 5.00 kg, Temperature 200 °C |
37 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Melt Flow | 37 g/10 min @Load 5.00 kg, Temperature 200 °C |
37 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7930-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Melt Flow | 37 g/10 min @Temperature 224 °C |
37 g/10 min @Temperature 435 °F |
ASTM D1238 |
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether.. |
|||
Melt Flow | 37 g/10 min @Load 2.16 kg, Temperature 380 °C |
37 g/10 min @Load 4.76 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-8102 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Melt Flow | 37 g/10 min @Load 10.0 kg, Temperature 220 °C |
37 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Melt Flow | 37 g/10 min @Load 10.0 kg, Temperature 220 °C |
37 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Melt Flow | 37 g/10 min @Load 10.0 kg, Temperature 300 °C |
37 g/10 min @Load 22.0 lb, Temperature 572 °F |
ASTM D570 |
LG Chemical LUCON PO6063 mPPO+CNT+CF+GF Description: Injection Molding, mPPO+CNT+CF+GF, Electrostatic Dissipation, High Strength, Low WarpageApplication: LCD Cell TrayCAS No. 35134-01-4, 65997-17-3, 7440-44-0 and 7782-42-5Information prov.. |
|||
Melt Flow | 37 g/10 min @Load 10.0 kg, Temperature 220 °C |
37 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical RX710 ABS, High Impact, Chemical Resistance to HCFC Feature: Injection Molding, Chemical Resistance to HCFC, High ImpactApplication: Refrigerator Dispensor & HomebarCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 37 g/10 min | 37 g/10 min | |
Intercontinental Polymers 555 PBT Polymer Elastomer Polyester Pellets Applications: Engineering Resin - ModifiedInformation provided by Intercontinental Polymers. |
|||
Melt Flow | 37 g/10 min @Load 5.00 kg, Temperature 260 °C |
37 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® BM 25 FN20 700350 Nylon 6, 25% Mineral PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen |
|||
Melt Flow | 37 g/10 min @Load 10.0 kg, Temperature 220 °C |
37 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
Styrolution NOVODUR® P2H-AT ABS, Injection Grade Standard injection molding grade, easy flow, high gloss, hard, antistatic.Applications: Telephones, household goods, video and audio industry, office equipment. |
|||
Melt Flow | 37 g/10 min @Load 2.16 kg, Temperature 230 °C |
37 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HH450FB Polypropylene Homopolymer HH450FB is a polypropylene homopolymer intended for fiber applications. Applications: HH450FB has been developed especially for applications like spunbonded nonwovens.Information provided by Boreal.. |
|||
Melt Flow | 37 g/10 min @Load 2.16 kg, Temperature 230 °C |
37 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HH450MO Polypropylene HH450MO is a polypropylene homopolymer intended for injection molding. This grade is especially suitable for high-speed injection molding of articles demanding easy flow. This polymer is a CR (cont.. |
|||
Melt Flow | 37 g/10 min @Load 5.00 kg, Temperature 224 °C |
37 g/10 min @Load 11.0 lb, Temperature 435 °F |
ASTM D1238 |
DSM Biomedical Elasthane™ 75D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Melt Flow | 37 g/10 min @Load 1.20 kg, Temperature 300 °C |
37 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 2256 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Melt Flow | 37 g/10 min @Load 1.20 kg, Temperature 300 °C |
37 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 2258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Melt Flow | 37 g/10 min @Load 2.16 kg, Temperature 190 °C |
37 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Diamond Polymers Softflex® 4550 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 37 g/10 min @Load 1.20 kg, Temperature 300 °C |
37 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® LED2245 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeFormerly Makrolon DP1-1857MVR (300 °C/1.2 kg) 36 cm3/10 minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
Melt Flow | 37 g/10 min @Load 5.00 kg, Temperature 280 °C |
37 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
Melt Flow | 37 g/10 min @Load 5.00 kg, Temperature 270 °C |
37 g/10 min @Load 11.0 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® DP C 1502 702353 PBT+PC
(discontinued **) PBT+PC, non-reinforced, injection molding, impact modified, low tendency to warp, UV-stabilized |
|||
Melt Flow | 37 g/10 min @Load 10.0 kg, Temperature 220 °C |
37 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 37 g/10 min @Load 2.16 kg, Temperature 270 °C |
37 g/10 min @Load 4.76 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® TP 740-201 000000 PBT + ASA, 20% Glass Fiber
(discontinued **) PBT+ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finish |