Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 260 °C |
33 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210HF is a 10% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low sh.. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 200 °C |
33 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 330 °C |
33 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 330 °C |
33 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 330 °C |
33 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: High Flow, Good StiffnessUses: Food containers, Small pails, Nursery containers |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
Estimated using room temperature density |
Ineos ABS Lustran® M203FC Standard impact strength, easy flowing, high gloss, BgVV and FDA quality for food contact. ,Property data per ISO test methods. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 290 °C |
33 g/10 min @Load 11.0 lb, Temperature 554 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 260 °C |
33 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 260 °C |
33 g/10 min @Load 4.76 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® B 3215 901510 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 280 °C |
33 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 280 °C |
33 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 280 °C |
33 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 266 °C |
33 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V8280 PBT+PET 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 250 °C |
33 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 250 °C |
33 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-3402F PC, 40% Glass Filled FR PC/GF material with 40% GF reinforcement that can be used in printer LSUInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BF-0930 MABS, Unreinforced Scratch Resistant Scratch resistantInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BF-0930 MABS, Unreinforced Scratch Resistant Scratch resistantInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 250 °C |
33 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2790C PPE+HIPS (Asia Pacific) PPE/HIPS unfilled FR-V1, 90C |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 266 °C |
33 g/10 min @Load 2.65 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 266 °C |
33 g/10 min @Load 2.65 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 266 °C |
33 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East) 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 250 °C |
33 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 506.07 Low Density Polyethylene Resin Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit.. |
|||
Melt Flow | 33 g/10 min | 33 g/10 min | ISO 1133 |
Domo 2340RC Polypropylene Copolymer Information provided by Domo. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HD 6733.17 Injection Molding Resin Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable .. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 230 °C |
33 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® HU 75 AV Polypropylene Impact Copolymer Description: CAPILENE® HU 75 AV is a nucleated and antistatic controlled rheology impact copolymer for injection molding. It is characterized by improved stiffness and medium impact resistance. .. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 230 °C |
33 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 30 cm<sup>3</sup>/10 min; ISO 1133 |
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 250 °C |
33 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |