Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 3.8 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 3.8 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.8 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Plaskolite West Optix® CP - 75 HID General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Polimeri Europa Edistir N 2560 Polystyrene
High molecular weight general purpose polystyrene with good mechanical strength and good thermal resistance. It is recommended for in-line forming of disposable packaging, for sheet extrusion in ble..
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Resirene Resirene® 6220 High Impact Polystyrene
Features:Low FlowEasy ProcessingGood GlossHigh ElongationFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Extrusion/ ThermoformingDisposablesGPPS/HIPS BlendsRefrigerator PartsInformation p..
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 8306 UV8D, 8306G UV8D MDPE Rotational Molding Resin  (discontinued **)
Features: Balanced combination of toughness, ESCR and processability.Applications: General purpose.Data provided by the manufacturer.
Melt Flow 3.8 g/10 min

@Load 10.0 kg,
Temperature 220 °C
3.8 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min.
Ineos ABS Centrex® 815 ASA Blend  (discontinued **)
Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye..
Melt Flow 3.8 g/10 min
3.8 g/10 min
ASTM D1238
LyondellBasell Alathon® M6138 High Density Polyethylene
ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness...
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
M. Holland Company PP204 Polypropylene Homopolymer
Features: Homopolymer, Low Residuals, Good Stiffness, Low Water CarryoverApprovals: FDA 21 CFR 177.1520Information provided by M. Holland.
Melt Flow 3.8 g/10 min
3.8 g/10 min
ASTM D1238
I. Stern N2560 General Purpose Crystal Polystyrene
Features:Excellent ClarityExcellent Process PropertiesHigh Heat MoldingApplicationsMedical PartsDomestic AppliancesAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St..
Melt Flow 3.8 - 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 - 5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC ST508 Linear Low Density Polyethylene, Cast Film Grade
Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica..
Melt Flow 3.8 g/10 min

@Load 21.6 kg,
Temperature 230 °C
3.8 g/10 min

@Load 47.6 lb,
Temperature 446 °F
ASTM D1238
Kureha KF Polymer 1550 High Viscosity PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Samsung Cheil Industries Starex® VC-0830 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Samsung Cheil Industries Starex® VC-0830 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 3.8 g/10 min

@Load 10.0 kg,
Temperature 250 °C
3.8 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL EXT130 PPE+HIPS (Asia Pacific)
PPE+PS for auto exterior, High heat
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 190 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
SCG Chemicals EL-Leneâ„¢ H570P High Density Polyethylene Pipe Resin
Key Characteristics: High stiffness, good processingRecommended Applications: Corrugated pipes, non pressure pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 140 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 284 °F
ISO 1133
Borealis Borcell™ HE4873 High Density Polyethylene
Borcell™ HE4873 is a fully formulated compound for physical foamed data cable insulation. Borcell™ HE4873 is a high-density polyethylene compound containing blowing agent for the production of foa..
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Total PSI 960E Polystyrene
Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids ..
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene™ LD 727.22 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 727.22 is a high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Availability: North America Additive: ..
Melt Flow 3.8 g/10 min

@Load 10.0 kg,
Temperature 220 °C
3.8 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Melt Volume Rate (ml/10 min); ISO 1133
Chi Mei Kibilac® PW-997S ASA Polymer
Extrusion
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LDPE LD 252 Low Density Polyethylene Resin (European Grade)
Product Description: LD 525 is a high purity LDPE extrusion coating grade, designed to meet environmental needs for reduced fume emissions during plastics conversion. This grade offers:Low volatiles..
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 175 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 347 °F
ASTM D1238
Diamond Polymers Softflex® 6538 Thermoplastic Elastomer Alloy, Clear
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 3.8 g/10 min

@Load 10.0 kg,
Temperature 220 °C
3.8 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Melt Volume Rate (ml/10 min); ISO 1133
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
High FDI; high heat
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem PB681 LDPE Cast and Blown Film Extrusion, Injection Molding Polyethylene
PB681 is a resin produced under high pressure in a tubular reactor. This resin presents excellent 'draw down' (stability to form fine films). The films produced with this resin have excellent optica..
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Braskem PB681/59 Blown Film Extrusion Low Density Polyethylene
Description: PB681/59 is a grade produced under high pressure in a tubular reactor. This resin is used for laminating films mainly on paper substrate. It is also used in the extrusion coating proces..
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Braskem PB681/59 LDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Lamination film; general purpose. Information provided by Braskem
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Braskem TI60035NB High Impact Copolymer Polypropylene
Description: Extra high izod impact, superior low temperature drop impact.Applications: Suggested uses include compounding, automotive, injection molding.Process: Injection Molding. This resin meets..
Melt Flow 3.8 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Iran Petrochemical (PCC) Arak 0640AA LLDPE  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Melt Flow 3.8 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.8 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Melt Flow 3.8 g/10 min

@Load 10.0 kg,
Temperature 250 °C
3.8 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL PX2630 PPE+HIPS (Asia Pacific)
PPE+HIPS Unfilled high Impact
Melt Flow 3.8 - 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.8 - 5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ineos Nova 610 Crystal Polystyrene GP Grade  (discontinued **)
Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe..
Copyright © lookpolymers.com All Rights Reserved