Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | ISO 60 |
Raschig Group EPOXIDUR® 3580 EP Epoxy Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod.. |
|||
Apparent Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | ISO 60 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Apparent Bulk Density | 0.600 - 1.01 g/cc | 0.0217 - 0.0365 lb/in³ | Average value: 0.750 g/cc Grade Count:3 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded
(discontinued **) This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 204 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok 204 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to accommodate a wide range of molding situations. In addition, it is recommended for use in thin wall .. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 5440 Black General Purpose Phenolic Molding Compound
(discontinued **) Plaslok 5440 is the replacement material for the former Union Carbide BMRS-5440. It is a two-stage, phenolic molding compound that has been successfully formulated to accommodate a very wide range .. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 7000 is the replacement material for the former Union Carbide BMM-7000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding and preheating characteristics.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Sumitomo Bakelite North America 775 CAF Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Tipco Megabatch® MD 3220 LLDPE based Metal De-Activator Masterbatch 20% Metal De-Activator (Cu-Inhibitor) Masterbatch in LLDPEApplications: General PurposeProcessing: Injection & ExtrusionInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Tipco Megabatch® UV 1022 Polypropylene based UV Stabilizer Masterbatch 20% UV Stabilizer (polymeric-HALS) Masterbatch in PP HomopolymerApplications: General PurposeProcessing: Injection & ExtrusionInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | TRM-37 |
Tipco Tipcolene® MD 3220 - Metal Deactivator (20% Copper Inhibitor) Masterbatch in LLDPE |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | TRM-37 |
Tipco Tipcolene® UV 1022 - Polymeric-HALS (20% UV Stabilizer) Masterbatch in Polypropylene Homopolymer |
|||
Apparent Bulk Density | 0.600 - 0.620 g/cc | 0.0217 - 0.0224 lb/in³ | ISO 60 |
Tisan TISMOSET® Properties:Flame retardantHigh gloss surfaceImproved thermal and electircal strengthHigh impact strengthMinimized shrinkage at the presence of moldingHigh melting flow indexReduced moisture absorpti.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Cytec Thornel® Mat VME Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 200 µm - inadequate for good mechanical property.. |
|||
Apparent Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Domo Domamid® 24 T Polyamide 6 DOMAMID® 24 T are a low viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Domamid T products are special textile grades with a high uniformity of relative viscosity and Amino.. |
|||
Apparent Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Domo Domamid® 24 T-HS Polyamide 6 DOMAMID® 24 T-HS are a low-viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Domamid®-T-products are special textile grades with a high uniformity of relative viscosity and .. |
|||
Apparent Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Domo Domamid® 2403 T-HS Polyamide 6 DOMAMID® 2403 T-HS are a low-viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Domamid®-T-products are special textile grades with a high uniformity of relative viscosity an.. |
|||
Apparent Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Domo Domamid® 28 Polyamide 6 DOMAMID® 28 are Polyamide 6 pellets produced from Caprolactam by polymerization.Applications: Textile yarn extrusionCompounding Injection moulding Information provided by Domo |
|||
Apparent Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Domo Domamid® 32 Polyamide 6 DOMAMID® 32 are Polyamide 6 pellets with a higher viscosity produced from Caprolactam by polymerization.Applications: Standard quality for production of monofilaments and fishing netsInformation pr.. |
|||
Apparent Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Domo Domamid® 33 Polyamide 6 DOMAMID® 33 are Polyamide 6 pellets with a higher viscosity produced from Caprolactam by polymerization. Applications: Standard quality for production of monofilaments and fishing netsInformation p.. |
|||
Apparent Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Domo Domamid® 27 Polyamide 6 DOMAMID® 27 are Polyamide 6 pellets produced from Caprolactam by polymerization.Applications: Textile yarn extrusionCompounding Injection moulding Information provided by Domo |
|||
Apparent Bulk Density | 0.600 - 0.680 g/cc | 0.0217 - 0.0246 lb/in³ | IS 867-1963 |
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Arkema Group Lacovyl® GB 1150 M PVC, Pipe Grade LACOVYL GB 1150 M is a vinyl chloride homopolymer produced by the Elf Atochem's mass polymerization process.Its characteristics are : Viscosity index (ISO 1628-2):112 ml/g,(K value:67). Apparen.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | Tap density |
Carborundum CarboTherm™ CTUF Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |
|||
Apparent Bulk Density | 0.600 - 0.660 g/cc | 0.0217 - 0.0238 lb/in³ | IS 867-1963 |
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Apparent Bulk Density | 0.600 - 0.860 g/cc | 0.0217 - 0.0311 lb/in³ | Average value: 0.732 g/cc Grade Count:6 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plaslok 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7000 is the replacement material for .. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plaslok 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
Apparent Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 83 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Switch covers, rolls, handle casings.. |