Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 110000 cP | 110000 cP | after 2 hours; ASTM D1084 |
Multibase SILASTIC® MDX4-4210 Dow-Corning Biomedical Grade Elastomer Information provided by Multibase |
|||
Viscosity | 110000 cP | 110000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Viscosity | 110000 cP | 110000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Viscosity | 110000 cP | 110000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Viscosity | 110000 cP | 110000 cP | Melt Viscosity, 280°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics NORYL PVX524 PPE PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT |
|||
Viscosity | 110000 cP | 110000 cP | Melt Viscosity, 250°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Viscosity | 110000 cP | 110000 cP | Melt Viscosity, 250°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Viscosity | 110000 cP | 110000 cP | Mixed (cp #52, 5 rpm) |
Tra-Con Supertherm 826M01 High Performance Diamond Epoxy Adhesive SUPERTHERM 826M01 is a one-part, smooth paste ULTRA HIGH THERMALLY CONDUCTIVE diamond filled epoxy adhesive recommended for semiconductor die-attach and other micro-electronic applications where the.. |
|||
Viscosity | 110000 - 345000 cP | 110000 - 345000 cP | Thixotropic |
Loctite® 5205 Flexible Cure Flange Sealant Anaerobic GasketingLoctite® 5205 Flexible Cure Flange SealantFast curing and flexible, good sealing properties against oil and water/glycol particularly at high temperatures. High viscosity. Recom.. |
|||
Viscosity | 110000 - 345000 cP | 110000 - 345000 cP | Thixotropic |
Loctite® 5206 Flexible Cure Flange Sealant Anaerobic GasketingLoctite® 5206 Flexible Cure Flange SealantSlow curing allows for micro-movement during assembly operations. Good sealing properties against oil and water/glycol. High viscosity... |
|||
Viscosity | 110000 cP | 110000 cP | catalyzed with QM 264B |
ACC QM 264 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 264 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin .. |