Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 300000 cP | 300000 cP | |
NextGen Adhesives P907-30 Optical Assembly Adhesive Description: NGAC P907-30 is a high viscosity, controlled flow encapsulant designed for microelectronics applications requiring low shrinkage and high reliability performance.Advantages and Applicat.. |
|||
Viscosity | 300000 cP @Shear Rate 190 1/s, Temperature 230 °C |
300000 cP @Shear Rate 190 1/s, Temperature 446 °F |
|
Noltex Soarnol® BG3522 Ethylene Vinyl Alcohol Copolymer Special designed high MFI grade. New EVOH for extrusion coating. Ethylene content 35 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, .. |
|||
Viscosity | 300000 cP @Temperature 25.0 °C |
300000 cP @Temperature 77.0 °F |
Uncured |
Permabond HH190 Anaerobic Gasketmaker Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the .. |
|||
Viscosity | 300000 cP @Temperature 400 °C |
300000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica.. |
|||
Viscosity | 300000 - 1.90e+6 cP @Temperature 190 - 190 °C |
300000 - 1.90e+6 cP @Temperature 374 - 374 °F |
Average value: 495000 cP Grade Count:22 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Viscosity | 300000 - 1.00e+6 cP | 300000 - 1.00e+6 cP | |
Lord Adhesives 309 General Purpose, Non-Sag, Thixotropic Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 300000 - 1.00e+6 cP | 300000 - 1.00e+6 cP | |
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 300000 - 400000 cP | 300000 - 400000 cP | Paste |
Lucas-Milhaupt Lucanex 616 Active Metal Brazing Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste |
|||
Viscosity | 300000 - 400000 cP | 300000 - 400000 cP | Paste |
Lucas-Milhaupt Lucanex 721 Active Metal Brazing Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste |
|||
Viscosity | 300000 cP @Shear Rate 206 1/s, Temperature 200 °C |
300000 cP @Shear Rate 206 1/s, Temperature 392 °F |
ASTM D3835 |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
Viscosity | 300000 cP @Temperature 25.0 °C |
300000 cP @Temperature 77.0 °F |
Mixed (cp #52, 1 rpm) |
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low.. |
|||
Viscosity | 300000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
300000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 1124 Modified EVA Adhesive Resin Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Viscosity | 300000 - 500000 cP | 300000 - 500000 cP | Dynamic |
Dow Corning 9041 Silicone Elastomer Blend A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, haircare, color cosmetics, suncare, antiperspirants and deodorants, and w.. |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® T65 HI PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature .. |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F130-C PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F130-E1 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F132 PA6 Film Extrusion, High Viscosity |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F132-C1 PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F132-E1 PA6 Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 300000 cP @Temperature 190 °C |
300000 cP @Temperature 374 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1377E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 300000 cP @Temperature 280 °C |
300000 cP @Temperature 536 °F |
DAM; @ 1000 sec-1; ISO 11443 |
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6
(Unverified Data**) 15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per.. |
|||
Viscosity | 300000 - 800000 cP | 300000 - 800000 cP | Part B |
Master Bond EP21TDC-2LO Two component, highly flexibilized epoxy resin compound Product Description: Master Bond Polymer System EP21TDC-2LO is a two component, highly flexible epoxy resin compound for high performance bonding, sealing, coating, and encapsulation. It is formulat.. |
|||
Viscosity | 300000 cP @Temperature 400 °C |
300000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |