Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 200000 cP @Temperature 400 °C |
200000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Viscosity | 200000 cP @Temperature 400 °C |
200000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Viscosity | 200000 cP @Temperature 400 °C |
200000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Viscosity | 200000 cP | 200000 cP | Part B, Spindle TD, 2.5 rpm; Uncured |
Resinlab® AR 4400 HP Metal & Composite Bonding Methacrylate Adhesive Resinlab™ AR 4400 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a.. |
|||
Viscosity | 200000 cP | 200000 cP | Spindle TD, 2.5 rpm; Curing |
Resinlab® AR 4400 HP Metal & Composite Bonding Methacrylate Adhesive Resinlab™ AR 4400 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a.. |
|||
Viscosity | 200000 - 260000 cP | 200000 - 260000 cP | |
Lord Adhesives Metech 3502 Palladium Silver Conductor Composition Designed for use in the manufacture of hybrid circuitry, resistor networks, potentiometers as well as general purpose microcircuitry. It employs a conventional glass bonding mechanism, has wide proc.. |
|||
Viscosity | 200000 - 260000 cP | 200000 - 260000 cP | |
Lord Adhesives Metech 3505 Palladium Silver Conductor Composition Designed for use in the manufacture of hybrid circuitry, resistor networks, potentiometers as well as general purpose microcircuitry. It employs a conventional glass bonding mechanism, has wide proc.. |
|||
Viscosity | 200000 cP | 200000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Viscosity | 200000 - 600000 cP | 200000 - 600000 cP | Part A |
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation .. |
|||
Viscosity | >= 200000 cP | >= 200000 cP | Part B |
Master Bond EP42HT-2ND-2Med Heat Resistant, Medical Grade Non-Drip Epoxy Master Bond Polymer System EP42HT-2ND2MED (Black) is a room temperature curable two component epoxy adhesive and sealant featuring high temperature resistance along with outstanding chemical resista.. |
|||
Viscosity | >= 200000 cP | >= 200000 cP | |
Master Bond EP65ND Fast Curing, High Shear Strength Epoxy This two component adhesive system is formulated to cure quickly at ambient temperatures e.g. 8-10 minutes, shorter lives at higher temperatures for maximum bond strength. Tensile lap shear strength.. |
|||
Viscosity | >= 200000 cP | >= 200000 cP | Part B |
Master Bond MasterSil 153Med Silicone Paste for Medical Applications Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it.. |
|||
Viscosity | 200000 cP @Shear Rate 100 1/s, Temperature 300 °C |
200000 cP @Shear Rate 100 1/s, Temperature 572 °F |
|
DuPont Selar® PA 3426 Nylon Barrier Resin Selar® PA 3426 is an amorphous nylon (polyamide) resin which exhibits superior transparency, good barrier properties to gases, water, solvents and essential oils and high temperature structural pro.. |
|||
Viscosity | 200000 cP | 200000 cP | Mixed (cp #51, 0.5 rpm) |
Tra-Con Tra-Bond 862-12 Information provided by Tra-Con Inc. |
|||
Viscosity | 200000 cP @Temperature 25.0 °C |
200000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 51 Two-Component General Purpose Epoxy Adhesive Emerson & Cuming 51 Eccobond® Two-Component General Purpose Epoxy AdhesiveFilled, general purpose epoxy adhesive. Used with a variety of catalysts. Excellent adhesion to a variety of metal, plastic.. |
|||
Viscosity | 200000 cP | 200000 cP | at 20 RPM |
Loctite® 332 Severe Environment Structural Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Viscosity | >= 200000 cP @Temperature 23.0 °C |
>= 200000 cP @Temperature 73.4 °F |
|
Master Bond EP3HTMED One Component, Biocompatible Epoxy System Master Bond Polymer System EP3HTMed combines the ease of a one part, no mix, fast curing adhesive with high shear strength. This special formulation fully meets USP Class VI requirements. EP3HTMed p.. |
|||
Viscosity | 200000 - 300000 cP | 200000 - 300000 cP | Part A |
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests Description: Master Bond Supreme 11AOHTLO is a two component epoxy resin system for high performance bonding and sealing. Although, it is formulated to cure at room temperature, the best cure schedu.. |
|||
Viscosity | 200000 cP | 200000 cP | dynamic |
Dow Corning 7-3099 DIMETHICONE HIP EMULSION A concentrated emulsion of Dimethicone (100 cSt) that is designed to facilitate the rapid development of skin care formulations which contain this emollient. Typical applications include: suncare, b.. |
|||
Viscosity | 200000 cP | 200000 cP | dynamic |
Dow Corning SE 4422 SILICONE RTV One-part, grey, moisture cure RTV, flowable, thermally conductive, UL V-1.Information provided by Dow Corning |
|||
Viscosity | 200000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
200000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® T65 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding, easy .. |
|||
Viscosity | 200000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
200000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Viscosity | 200000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
200000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® XP32-E1 PA6 Film Extrusion, Medium Viscosity, Lubricated, Nucleated |
|||
Viscosity | 200000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
200000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® XP36-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 200000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
200000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® FR630 GR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Viscosity | 200000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
200000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity | 200000 cP | 200000 cP | uncured |
Atom Adhesives AA-DUCT 904 Epoxy Adhesive AA-DUCT 904 is a single component, heat curing, conductive epoxy that was designed for ease in handling. This high performance conductive epoxy cures quickly at elevated temperatures making it ideal.. |
|||
Viscosity | 200000 - 700000 cP @Temperature 400 - 420 °C |
200000 - 700000 cP @Temperature 752 - 788 °F |
Average value: 445000 cP Grade Count:13 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |