Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs R00 ABS, High Impact Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC K5025 PP, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF5020 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Europe-Africa-Middle East) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS7R PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC K5040 E30 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF5030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH MGF5040 Polypropylene Homopolymer, Multifiller Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 195-1336 LMDPE Rotational Molding Resin Description: ICORENE 195-1336 is a compounded linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and sti.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 315 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 599 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched (Europe-Africa-Middle East) LNP* Lubricomp* OCL4036 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Asia Pacific) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 280 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX954 PPE+PA (Europe-Africa-Middle East) NORYL GTX954 is an unfilled grade with improved processability and optimised heat/impact balance. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 300 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 300 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Melt Index of Compound | 5.0 g/10 min @Load 1.20 kg, Temperature 280 °C |
5.0 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Melt Index of Compound | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim.. |
|||
Melt Index of Compound | 5.0 g/10 min | 5.0 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Melt Index of Compound | 5.0 g/10 min | 5.0 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |
|||
Melt Index of Compound | 5.0 - 8.0 g/10 min | 5.0 - 8.0 g/10 min | ASTM D1238 |
Cheng Yu Plastic VH825 Flame Retardant ABS, Medium Impact |
|||
Melt Index of Compound | 5.0 g/10 min @Load 21.6 kg, Temperature 150 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 302 °F |
Fainplast |
Fainplast Compounds HAX HF 018/33 Halogen Free PVC Sheathing, high flexibility |
|||
Melt Index of Compound | 5.0 g/10 min @Load 21.6 kg, Temperature 150 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 302 °F |
Fainplast |
Fainplast Compounds HAX HF 22 Halogen Free PVC Sheathing; standard grade for power and special cables |
|||
Melt Index of Compound | 5.0 - 14 g/10 min @Load 5.00 kg, Temperature 265 °C |
5.0 - 14 g/10 min @Load 11.0 lb, Temperature 509 °F |
|
3M Dyneon™ Dynamar™ FX 5911 Polymer Processing Additive Dynamar FX 5911 is a free-flowing fluoropolymer processing aid that is designed for use at very low levels (typically 250-1000 ppm) necessary to improve processing, it does not alter or detract from.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF5035 PD2 VT Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled/Heat Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH TS5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |