Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 250 °C |
11 g/10 min @Load 2.65 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® OQ1026 PC (Asia Pacific) LEXAN OQ1026 is an optical quality, high purity PC resin optimized for the demanding short cycle times used in DVD production. Advances in technology further enhanced the processability while mainta.. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 200 °C |
11 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238G |
Total Finaclear® 530 Clear Impact Polystyrene
(discontinued **) Finaclear® 530 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with other.. |
|||
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 3262R PC (Asia Pacific) Lexan* 3262R Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V2@1.5mm rating and is available .. |
|||
Melt Index of Compound | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 360 °C |
11 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 360 °C |
11 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 360 °C |
11 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 300 °C |
11 g/10 min @Load 4.76 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8141 PC (Asia Pacific) LNP* Thermocomp* EXTC8141 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Melt Index of Compound | 11 g/10 min @Load 10.0 kg, Temperature 300 °C |
11 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH5120 PPE+PS Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re.. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific) Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 260 °C |
11 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Europe-Africa-Middle East) PPX7110 is an alloy of PP and PPO, providing high impact and good heat resistance. Generic identification acc. ISO11469: >PP+PPE+PS-I |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Melt Index of Compound | 11 - 15 g/10 min @Load 2.16 kg, Temperature 250 °C |
11 - 15 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Shinkong Synthetic Fibers Shinite® D201K011 PBT, Super Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Melt Index of Compound | 11 g/10 min @Load 10.0 kg, Temperature 300 °C |
11 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Melt Index of Compound | 11 g/10 min @Load 10.0 kg, Temperature 300 °C |
11 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Melt Index of Compound | 11 g/10 min @Load 8.70 kg, Temperature 190 °C |
11 g/10 min @Load 19.2 lb, Temperature 374 °F |
ASTM D1238 |
Advanced Polymer Alloys DuraGrip™ 6165 TR Thermoplastic Elastomer DuraGrip® DGR6165TR is a translucent thermoplastic elastomer (TPE) formulated for excellent elastic properties and enhanced adhesion to engineered thermoplastics using insert molding, co-injection .. |
|||
Melt Index of Compound | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |