Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.012 cm/cm @Thickness 6.35 mm |
0.012 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-60/TC/20 Polypropylene Homopolymer, 20% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 - 0.014 cm/cm @Thickness 3.17 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 cm/cm @Thickness 6.35 mm |
0.012 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-61/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 cm/cm @Thickness 6.35 mm |
0.012 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 - 0.014 cm/cm @Thickness 3.17 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 cm/cm @Thickness 6.35 mm |
0.012 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 cm/cm @Thickness 6.35 mm |
0.012 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 cm/cm @Thickness 3.17 mm |
0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 - 0.021 cm/cm @Thickness 1.60 mm |
0.012 - 0.021 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 2000-104D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Linear Mold Shrinkage | 0.012 - 0.021 cm/cm @Thickness 1.60 mm |
0.012 - 0.021 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 2000-201D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm @Thickness 3.00 mm |
0.012 - 0.016 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.012 - 0.014 cm/cm @Thickness 3.00 mm |
0.012 - 0.014 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.012 cm/cm @Temperature 240 °C |
0.012 in/in @Temperature 464 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Linear Mold Shrinkage | 0.012 cm/cm @Temperature 240 °C |
0.012 in/in @Temperature 464 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 160 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Linear Mold Shrinkage | 0.012 cm/cm @Temperature 240 °C |
0.012 in/in @Temperature 464 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 95 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |