Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0090 - 0.010 cm/cm @Thickness 3.17 mm |
0.0090 - 0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm @Thickness 1.00 mm |
0.0070 - 0.010 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm @Thickness 1.00 mm |
0.0070 - 0.010 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.00 mm |
0.0060 - 0.010 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm @Thickness 1.00 mm |
0.0070 - 0.010 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.010 cm/cm @Thickness 1.60 mm |
0.0050 - 0.010 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PET 9130-200 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |