Polymer Property : Linear Mold Shrinkage = 0.010 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0090 - 0.010 cm/cm
<br>@Thickness 3.17 mm
0.0090 - 0.010 in/in
<br>@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.010 in/in
<br>@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.010 in/in
<br>@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.010 in/in
<br>@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
<br>@Thickness 1.00 mm
0.0070 - 0.010 in/in
<br>@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
<br>@Thickness 1.00 mm
0.0070 - 0.010 in/in
<br>@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
<br>@Thickness 3.00 mm
0.0060 - 0.010 in/in
<br>@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.010 in/in
<br>@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.010 in/in
<br>@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.010 in/in
<br>@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
<br>@Thickness 1.00 mm
0.0070 - 0.010 in/in
<br>@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0050 - 0.010 cm/cm
<br>@Thickness 1.60 mm
0.0050 - 0.010 in/in
<br>@Thickness 0.0630 in
vertical; ASTM D955
Gromax CCP PET 9130-200 30% Glass Filled
Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell..