Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0205 - 0.0225 cm/cm | 0.0205 - 0.0225 in/in | |
LATI Latan 13 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Transverse | 0.0205 - 0.0225 cm/cm | 0.0205 - 0.0225 in/in | |
LATI Latan 2 POM Polyoxymethylene (POM). Unfilled. High viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.0225 cm/cm | 0.020 - 0.0225 in/in | |
LATI Latan 23UV POM Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Linear Mold Shrinkage, Transverse | 0.0205 - 0.0225 cm/cm | 0.0205 - 0.0225 in/in | |
LATI Latan 9 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Transverse | 0.0205 - 0.0225 cm/cm | 0.0205 - 0.0225 in/in | |
LATI Latilub 73/13-01M POM, Molybdenum disulphide Filled Self-lubricating product based on Polyoxymethylene (POM). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |
|||
Linear Mold Shrinkage, Transverse | 0.0205 - 0.0225 cm/cm | 0.0205 - 0.0225 in/in | |
LATI Latiohm 73/23-10 CNT POM Semiconductive/dissipative product based on Polyoxymethylene (POM). Carbon nanotubes.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Transverse | 0.0205 - 0.0225 cm/cm | 0.0205 - 0.0225 in/in | |
LATI Latishield 73/13-07A POM, Steel Fiber Reinforced EMI shielding product based on Polyoxymethylene (POM). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |
|||
Linear Mold Shrinkage, Transverse | 0.0205 - 0.0225 cm/cm | 0.0205 - 0.0225 in/in | |
LATI Latistat 73/13-06 POM Dissipative product based on Polyoxymethylene (POM). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |