Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Thickness 2.00 mm |
0.016 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® S650FR BK851 PBT
(Unverified Data**) Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Thickness 2.00 mm |
0.016 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**) Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
5" x 0.5" x 0.125" bar; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.017 cm/cm | 0.016 - 0.017 in/in | ASTM D955 |
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Time 86400 sec |
0.016 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY UX98388 PPA LNP LUBRILOY* UX98388 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | Eurotec |
Eurotec® Tecomid® NA40 NL IM PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)
(Unverified Data**) Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 906 UR POM Copolymer unreinforced, impact modified POM-IInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Thickness 2.00 mm |
0.016 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, Conditioned Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, Conditioned Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.030 cm/cm @Time 86400 sec |
0.016 - 0.030 in/in @Time 24.0 hour |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Thickness 2.00 mm |
0.016 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 41 Nylon 66, Conditioned Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, Conditioned Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, Conditioned Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, Conditioned Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Thickness 2.00 mm |
0.016 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |