Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 6821 BLK This product is based on Kraton G and PP suitable for automotive applications and meets GM, Ford, and Chrysler specifications. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ASTM D955 |
PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | |
Polyplastic Armlen® PP MF 20-3IM Impact Modified Polypropylene Impact modified polypropylene composite materialInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO 294-4 |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
DuPont Performance Polymers Crastin® SK615SF NC010 PBT
(Unverified Data**) Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ASTM D955 |
LG Chemical LUPOL TE-5108 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Flow LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 1.00 mm |
0.011 in/in @Thickness 0.0394 in |
|
Kuraray Genestarâ„¢ TA104 Nylon Reinforced injection grade.Main Features:High reflectivityLess color change by heat and lightHigh reliabilityExample of applications:LED reflectors |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | 60x60x2; 270°C / WZ 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East) XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | |
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | DIS 294-4 |
Wellman Wellamid® GF1398-BK1 Nylon 66, 30% Glass Fiber Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecodur® PB70 GR15 NL100 PBT, 15% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | |
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecomid® NA40 KG30 NL 0B PA6.6, 30% glass fiber/glass bead reinforced, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.011 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.011 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® MX 1205 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MX 1205 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arke.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, Conditioned Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecomid® NB40 KG30NL IX PA6, 30% glass fiber/glass bead reinforced, impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |