Linear Mold Shrinkage, Transverse 0.025 - 0.027 cm/cm

@Time 86400 sec
0.025 - 0.027 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT
Health care grade, PTFE and silicone lubricated
Linear Mold Shrinkage, Transverse 0.025 - 0.027 cm/cm

@Time 86400 sec
0.025 - 0.027 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal
LNP LUBRILOY* KL201 is a compound based on Acetal resin containing Proprietary Lubricant. PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.025 - 0.027 cm/cm

@Time 86400 sec
0.025 - 0.027 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Asia Pacific)
LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.025 - 0.027 cm/cm

@Time 86400 sec
0.025 - 0.027 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East)
LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.024 - 0.027 cm/cm

@Thickness 3.20 mm
0.024 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 337 PBT
Low temperature impact PBT. Automotive applications: underhood power distribution boxes and covers.
Linear Mold Shrinkage, Transverse 0.021 - 0.027 cm/cm

@Thickness 3.20 mm
0.021 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Linear Mold Shrinkage, Transverse 0.021 - 0.027 cm/cm

@Thickness 3.20 mm
0.021 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Linear Mold Shrinkage, Transverse 0.021 - 0.027 cm/cm

@Thickness 3.20 mm
0.021 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® IQ3001 PBT
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Linear Mold Shrinkage, Transverse 0.021 - 0.027 cm/cm

@Thickness 3.20 mm
0.021 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific)
Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications.