Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.014 - 0.015 cm/cm | 0.014 - 0.015 in/in | ASTM D955 |
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | 0.125"x0.5"x5" bar; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.015 cm/cm @Thickness 3.18 mm |
0.013 - 0.015 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Linear Mold Shrinkage, Transverse | 0.0125 - 0.015 cm/cm | 0.0125 - 0.015 in/in | |
LATI Latamid 6 E02 PA 6, Impact modified Polyamide 6 (PA6). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A... |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Later 4 G/20 PBT, 20% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | |
LATI Latigray 52/11-01 CX/70 PP Homopolymer Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latilub 57-10T Y/15 PPA, Aramid Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Transverse | 0.0125 - 0.015 cm/cm | 0.0125 - 0.015 in/in | |
LATI Latistat 63-08 PA6, Impact Modified Dissipative product based on Polyamide 6 (PA6), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.015 cm/cm @Thickness 3.18 mm |
0.013 - 0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® F602G30 Nylon 66, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® N602G6S Nylon 66, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® F602G30 Nylon 66, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.015 cm/cm @Time 86400 sec |
0.010 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf R1000EI2 PA 66 (Europe-Africa-Middle East) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm @Thickness 3.20 mm |
0.012 - 0.015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm @Thickness 3.20 mm |
0.012 - 0.015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Asia Pacific) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm @Thickness 3.20 mm |
0.012 - 0.015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Europe-Africa-Middle East) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | DIS 294-4 |
Wellman Wellamid® GF33-66 22LH-NBK1 Nylon 66, 33% Glass Fiber Reinforced, General Purpose Grade All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0135 - 0.015 cm/cm | 0.0135 - 0.015 in/in | ISO DIS 294-4 |
Wellman Wellamid® GS1684-WBK1 25% Glass Sphere Filled Nylon 66 Description: Glass Sphere Filled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ISO DIS 294-4 |
Wellman Wellamid® GSF25/15-66 22L-NBK1 40% Glass Sphere/Fiber Reinforced Nylon 66 Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | DIS 294-4 |
Wellman Wellamid® MR409 22H-NBK1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ISO DIS 294-4 |
Wellman Wellamid® MR410 22H-GY1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latimass 53-04 D008 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
Solvay TECHNYL® 1011R PA6, DRY Description: Polyamide 6, Unfilled, lubricated, for injection molding. Available in: Asia Pacific Product Applications: TECHNYL® 1011R is used in all sectors of industry, offering an excellent flow.. |