Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Plastcom SLOVALEN PH 99 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
LNP Lubricomp® LL-4040 Polyetheretherketone, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE25-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE30-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 150x105x3, 260°C / MT 80°C; 500 bar; acc. ISO 2577 |
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 246M PA66, DRY Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.021 cm/cm | 0.019 - 0.021 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA) Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
Teknor Apex Monprene® MP-1277A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 208KBK-10N-L PA66, DRY Description: Polyamide 66, highly UV-resistance, toughness modified for injection molding.Available in: Asia PacificProduct Applications: TECHNYL A 208K BK 10N-L is used in all sectors of industry, .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 216 NATURAL FA PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1482-BK High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1606-N Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers with very low VOC emissions .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers pigmented red with very .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 2577 |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 2577 |
BASF Ultraform® N2720 M210 POM Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF |