Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Thickness 3.18 mm |
0.0045 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Trilliant™ HC X THC 1101 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Time 86400 sec |
0.0045 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Time 86400 sec |
0.0045 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Europe-Africa-Middle East) LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Time 86400 sec |
0.0045 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Time 86400 sec |
0.0045 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm | 0.0045 in/in | LATI |
LATI LARPEEK 50 G/60 60% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm | 0.0045 in/in | LATI |
LATI LAPEX A G/30 30% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3412HF PC 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Lastilac SP G/17 ABS, Glass Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0070 cm/cm | 0.0045 - 0.0070 in/in | |
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0070 cm/cm | 0.0045 - 0.0070 in/in | |
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0070 cm/cm | 0.0045 - 0.0070 in/in | |
LATI Laramid CE/60 PPA, 60% Mineral Reinforced Semi-aromatic polyamide (PPA) based compound. Mineral filler. High dimensional stability. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0060 cm/cm | 0.0045 - 0.0060 in/in | |
LATI Lasulf G/30 PSU, 30% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0085 cm/cm | 0.0045 - 0.0085 in/in | |
LATI Laticonther 52/11 GR/70 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0070 cm/cm | 0.0045 - 0.0070 in/in | |
LATI Laticonther 62 CPG/500 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0070 cm/cm | 0.0045 - 0.0070 in/in | |
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Latilub 87/28-12T G/20 PC, 20% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0055 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0055 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem 2313 PEI 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region... |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0055 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0055 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm | 0.0045 in/in | |
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Thickness 3.00 mm |
0.0045 in/in @Thickness 0.118 in |
|
Toyobo T-422-02R Nylon, Mineral-Reinforced Key Feature: High heat distortion and good toughness, high flowInformation provided by Toyobo Co., Ltd |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Thickness 3.00 mm |
0.0045 in/in @Thickness 0.118 in |
|
Toyobo T-423 Nylon, Mineral-Reinforced Key Feature: High heat distortion and good toughness, good surfaceInformation provided by Toyobo Co., Ltd |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm | 0.0045 in/in | |
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3412HF PC (Asia Pacific) 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm | 0.0045 in/in | 24 hrs; ISO 294 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |