Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93.5
93.5
ASTM D785
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Izod Impact, Notched 0.603 J/cm
1.13 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
232 °F
ASTM D648
Flammability, UL94 HB
HB