Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ISO 1183 |
Raschig Group AMPLA® 2500 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat.. |
|||
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ISO 1183 |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Specific Gravity | 1.50 - 1.70 g/cc | 1.50 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Specific Gravity | 1.50 - 1.70 g/cc | 1.50 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Specific Gravity | 1.50 - 1.70 g/cc | 1.50 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 150 MF Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr.. |
|||
Specific Gravity | 1.50 - 1.70 g/cc | 1.50 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 152 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Specific Gravity | 1.50 - 1.70 g/cc | 1.50 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Specific Gravity | 1.50 - 1.70 g/cc | 1.50 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 182 MF Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf.. |
|||
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Specific Gravity | 1.60 - 1.70 g/cc @Thickness 1.57 mm |
1.60 - 1.70 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP545 Carbon Fiber
(discontinued **) Description: NP545 is composed of carbon fiber fabric and an epoxy resin system. It has excellent moisture resistance and physical properties. Potential uses include fixtures and gage systems, high .. |
|||
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ASTM D1475 |
Lotus Nano Paint NAX 01 Tow-Component Nano-paint Description: More durable and specific application methods. This paint is suitable for traffic signs on the road, cross-walks, warning vibrating lines and limited lot marking. Related machines could.. |
|||
Specific Gravity | 1.65 - 1.70 g/cc | 1.65 - 1.70 g/cc | ASTM D792 |
Loxim 230 12V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Specific Gravity | 1.67 - 1.70 g/cc | 1.67 - 1.70 g/cc | ISO 12086 |
Isoflon ECTFE Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Specific Gravity | 1.64 - 1.70 g/cc | 1.64 - 1.70 g/cc | ASTM D 792 |
Karina 18/219-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.65 - 1.70 g/cc | 1.65 - 1.70 g/cc | ASTM D792 |
Loxim 230 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Specific Gravity | 1.66 - 1.70 g/cc | 1.66 - 1.70 g/cc | ASTM D-792 |
Axiall H 3138A Plenum Flexible PVC Plenum-grade Category 3 jacket. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.68 - 1.70 g/cc | 1.68 - 1.70 g/cc | ASTM D792 |
Adamas Adalon® 466 PTFE, Mineral/Organic Filler Information provided by Adamas, HPM |
|||
Specific Gravity | 1.65 - 1.70 g/cc | 1.65 - 1.70 g/cc | ASTM D792 |
Adamas Adalon® 266 PTFE, Mineral/Glass Bubbles Filler Information provided by Adamas, HPM |