Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall H 3138A Plenum Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Plenum-grade Category 3 jacket. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.66 - 1.70 g/cc
1.66 - 1.70 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 50 - 56
50 - 56
delayed; ASTM D-2240
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D-638
Elongation at Yield 255.8 %
255.8 %
Air Aging: 7 days @ 100°C; 75-mil plaques; UL 1581
275 %
275 %
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -6.00 °C
21.2 °F
ASTM D-746
Oxygen Index 51 %
51 %
ASTM D-638
Electrical Properties Metric English Comments
Dielectric Constant 3.67

@Frequency 1e+6 Hz
3.67

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F