| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| Nylene® Vexel™ B12GF45 SA , 45% Glass Reinforced PBT Description: Vexel™ B12GF45 SA is a 45% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | |
| Reliance Industries PET - 35% Glass filled Information provided by Reliance Industries |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| PolyOne Maxxam™ FR PO Conc 62 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ISO 1183 |
| Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ISO 1183 |
| Lehmann & Voss LUVOCOM® 3-8437 Polyamide 6, with glass fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Emergency running property.Suitable for metall inserts.Control.. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ISO 1183 |
| Gromax BFG50-FU00B3 Nylon 6 49.4% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
| Specific Gravity | 1.67 - 1.71 g/cc | 1.67 - 1.71 g/cc | ASTM D792 |
| Loxim 235 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D 792 |
| SABIC Innovative Plastics LNP Lubricomp OFG26XXP PPS - Linear LNP* Lubricomp* OFG26XXP is a compound based on Linear PPS containing Glass Fiber and Graphite Powder. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D 792 |
| SABIC Innovative Plastics Valox® EF4530 PBT (Asia Pacific) Easy flow, 30% glass-reinforced, PBTP resin. Flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| Shinkong Synthetic Fibers Shinite® T101G45 PET, 45% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | |
| Silberline Tufflake® 4850 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| Shinkong Synthetic Fibers Shinite® N602G6S Nylon 66, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
| Specific Gravity | 1.67 g/cc @Temperature 25.0 °C |
1.67 g/cc @Temperature 77.0 °F |
|
| Dow Corning LSPBK 22 SILICONE MASTERBATCH Information provided by Dow Corning |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | |
| Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, .. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| Techmer Lehvoss Compounds Luvotech™ J-1305/40 NAT PPS
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
| Specific Gravity | 1.67 - 1.73 g/cc | 1.67 - 1.73 g/cc | NBR NM-IEC 60811-1-3 |
| Karina 38/49-FC-LMP Straw Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
| Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
| Techmer Lehvoss Compounds Luvotech™ J-1305/40 BK5011 PPS
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||