Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D792 |
S&E Specialty Polymers G-4785E PVC Application: Flexible, PVC material designed for general-purpose extrusion applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.40 - 1.50 g/cc | 1.40 - 1.50 g/cc | |
PolyChem Alloy AquaGard™ 6004 AquaGard products are designed to improve the flame retardency of polyolefins without the use of halogen additives, such as bromine or chlorine. AquaGard products are available in a polyethylene .. |
|||
Specific Gravity | 1.40 - 1.50 g/cc | 1.40 - 1.50 g/cc | |
PolyChem Alloy AquaGard™ 6005M AquaGard products are designed to improve the flame retardency of polyolefins without the use of halogen additives, such as bromine or chlorine. AquaGard products are available in a polyethylene .. |
|||
Specific Gravity | 0.900 - 1.50 g/cc | 0.900 - 1.50 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 0862 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Extruded onlyRoHS CompliantInformation provided by Chomerics |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | |
Raschig Group PiMC 1221 High gloss PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | |
Raschig Group PiMC 1249 Sanitary, mix color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | |
Raschig Group PiMC 1253 Highly flame retardant This FR PiMC grade has been developed for top coats over M1 SMC/BMC grades. Such combinations will meet Europe’s most stringent FR tests for interiors of rolling stock, such as BS 476 and Spanish E.. |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | |
Raschig Group PiMC 1841 Metallic colors Adding metallic effect pigments to powder coatings gave rise to several application problems such as “spitting”. Synres-Almoco’s Metallic PiMC 1841 ensures easy processing and homogeneous surface.. |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | |
Raschig Group PiMC 1949 Granite colors PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Specific Gravity | 1.40 - 1.50 g/cc @Thickness 1.57 mm |
1.40 - 1.50 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP192 Synthetic Fabric
(discontinued **) Description: 8 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high tempe.. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E CAK 60-48/1-F Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E CAK 65-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.43 - 1.50 g/cc | 1.43 - 1.50 g/cc | ASTM D 792 |
Karina E CAK 85-48/1 Black PVC Compound Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.45 - 1.50 g/cc @Thickness 1.57 mm |
1.45 - 1.50 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP329 Cotton Fabric Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, .. |
|||
Specific Gravity | 1.40 - 1.50 g/cc @Temperature 25.0 °C |
1.40 - 1.50 g/cc @Temperature 77.0 °F |
|
Lord Adhesives Circalokâ„¢ 6031 A/B Epoxy Encapsulant Circalokâ„¢ 6031 A/B is a two-part epoxy potting compound with excellent electrical properties at elevated temperatures. Good arc-track resistance under high voltage loading and other dielectric .. |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | ASTM D 792 |
Karina 804-48/1-CRE Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina CAK 65-48/1-EX Black PVC Compound Reclaimed PVC compound recommended for foamed soles injection.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 47/35-GI Silver MBATCH for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 704-35/1-J-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 800-10/1-A-RT PVC Compound White Color Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 813-18/190-Y-RT-PO Gray PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 854-10/150-A-ERYB White PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 854-35/1-A-ERYB Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | IEC 1212-2 8.1 |
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm). Arc and tracking resistant.Information provided by Hippe. |
|||
Specific Gravity | 1.46 - 1.50 g/cc | 1.46 - 1.50 g/cc | ASTM D-792 |
Axiall 8840 Moldings & Extrusions Flexible PVC Economical general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.46 - 1.50 g/cc | 1.46 - 1.50 g/cc | ASTM D-792 |
Axiall 22951 Coax & Telecom Flexible PVC Non-lead stabilized, 75C rated jacket compound suitable for riser constructions over HDPE.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.46 - 1.50 g/cc | 1.46 - 1.50 g/cc | ASTM D-792 |
Axiall 8757 Moldings & Extrusions Flexible PVC Soft, general purpose, highly filled extrusion compound recommended for cove base moldings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.10 - 1.50 g/cc | 1.10 - 1.50 g/cc | ASTM D792 |
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding.. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 841-08/184-A-ERYB Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |