Polymer Property : Specific Gravity = 2.20 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.20 - 2.80 g/cc
2.20 - 2.80 g/cc
Parker Chomerics CHO-BOND 589-29 Conductive Epoxy
Low cost, highly conductive adhesive system which combines the strong adhesion characteristics of an epoxy with the superior conductivity of silver. CHO-BOND 589-29 adhesive meets the most exacting ..
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D792
Parker Chomerics CHO-BOND® 584-29 SYRINGE-PAK™ Silver Filled Conductive Epoxy and Hardener
Description: Chomerics CHO-BOND 584-29 is a two-component, highly conductive adhesive system that combines the strong adhesive characteristics of epoxy with the superior conductivity of pure silver...
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D792
Parker Chomerics CHO-FORM 5537 EMI Shielding Material
Fast Curing Form-in-Place EMI Shielding Material. Cho-Form 5537 is a one component, moisture cured, electrically conductive, form-in-place EMI gasketing material. The formulation contains nickel-pla..
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D395
Parker Chomerics CHOFORM® 5550 Conductive Form-in-Place Gasket
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Specific Gravity 2.20 g/cc
2.20 g/cc
125°C for 1,000 hrs; JIS-K-6220; ASTM D 792
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone
Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p..
Specific Gravity 2.20 g/cc
2.20 g/cc
Shandong Dongyue Polymer DF-201 PTFE Fine Powder
Usage: It is suitable for making unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse..
Specific Gravity >= 2.20 g/cc
>= 2.20 g/cc
Shandong Dongyue Polymer DF-202 PTFE Fine Powder
Usage: It is mainly used to process, belt, thin sheet and unsintered tape, thin wall rod etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF..
Specific Gravity <= 2.20 g/cc
<= 2.20 g/cc
Shandong Dongyue Polymer DF-203 PTFE Fine Powder
Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside...
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA)
LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber.
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D-792
Saint-Gobain Norton® F710 Chemically Resistant Skived PTFE Sheet
Description: PTFE = polytetrafluoroethyleneApplications include: Chemical Resistant; Common in Electrical/ElectronicsInformation provided by Saint Gobain Performance Products.
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D-792
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.002" thick)
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet..
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D-792
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.003" thick)
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet..
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D-792
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.005" thick)
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet..
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D-792
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.010" thick)
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet..
Specific Gravity 2.20 g/cc
2.20 g/cc
Cured
Tra-Con Tra-Bond 933-2 Moisture Resistant Chip Encapsulant
TRA-BOND 933-2 one component, highly filled, electrically insulating epoxy encapsulant is designed for encapsulating microelectronic chips. This epoxy provides excellent environmental and mechanical..
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D792
Ecomass® 4703BI62 Filled Polyurethane, Injection Molding
Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, radiation shielding applicationsInfor..
Specific Gravity 2.20 g/cc
2.20 g/cc
Daikin POLYFLON L-2 PTFE Low Polymer, White Fine Powder
White fine powder.Major Uses: Suited especially to applications requiring fine dispersion of particles. Mold lubrication/separation compounding agent for dry lubricants, paints, plastics, rubber, p..
Specific Gravity 2.20 g/cc
2.20 g/cc
Daikin POLYFLON L-5F PTFE Low Polymer, White Fine Powder
White fine powder.Major Uses: Extreme pressure additive and lubrication/separation compounding agent for dry lubricants, paints, plastics, rubber, etc.Information provided by Daikin Industries.
Specific Gravity 2.20 g/cc
2.20 g/cc
Daikin POLYFLON LDW-40 PTFE Low Polymer, Milky Liquid
Milky liquid.Major Uses: Additive to give water repellency to water base paints.Information provided by Daikin Industries.
Specific Gravity 2.20 g/cc
2.20 g/cc
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic..
Specific Gravity 2.20 - 2.23 g/cc
2.20 - 2.23 g/cc
ASTM D792
Adamas Adalon® 215 PTFE, 17% Glass Filled, Blue
Information provided by Adamas, HPM
Specific Gravity 2.20 g/cc
2.20 g/cc
Asahi Glass Fluon® CD076 PTFE Coagulated Dispersion Powder
Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc.