Daikin POLYFLON L-2 PTFE Low Polymer, White Fine Powder

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Daikin Industries
Trade Name POLYFLON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Daikin POLYFLON L-2 PTFE Low Polymer, White Fine Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
White fine powder.Major Uses: Suited especially to applications requiring fine dispersion of particles. Mold lubrication/separation compounding agent for dry lubricants, paints, plastics, rubber, printing inks, etc. and extreme pressure additive for oil and grease.Information provided by Daikin Industries.
Physical Properties Metric English Comments
Specific Gravity 2.20 g/cc
2.20 g/cc
Bulk Density 0.370 g/cc
0.0134 lb/in³
Particle Size >= 5.0 µm
>= 5.0 µm
Average
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
PTFE Component
Oxygen Index >= 95 %
>= 95 %
PTFE Component
Electrical Properties Metric English Comments
Dielectric Constant 2.1

@Frequency 1000 Hz
2.1

@Frequency 1000 Hz
PTFE Component; ASTM D150
2.1

@Frequency 1e+6 Hz
2.1

@Frequency 1e+6 Hz
PTFE Component; ASTM D150
Dissipation Factor 0.00010 - 0.00022
0.00010 - 0.00022
PTFE Component