Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced Polycarbonate, 40% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 19-7669 Polyamide 46, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Lucent Polymers LPB-130 Polybutylene Terephthalate, 30% Glass Fiber/Mineral Reinforced, Low Warp Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | |
Sylvin Technologies 8960-95 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6 LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® K4560 PBT 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® VC130 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 LNP* THERMOCOMP* RF-1008 is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Chase Plastics CP Pryme® N340HSL (COND, 50% RH) Nylon 6 (Utility Grade), 40% Glass Fiber Reinforced, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Brown 1281 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 1281 is a brown color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | |
Trelleborg Commercial Neoprene® C798 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Diamond Polymers DIAMALOY 508 30% Glass Filled PC/Polyester Alloy, UV Stabilized Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Asahi Kasei Thermylene® P6-30FG-0570 30% Glass Fiber Reinforced, Flame Retardant Information provided by Asahi Thermofil |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | @ 25°C |
ACC EP MAP-Z 14 EPI Engineered Polymers Aliphatic Polymer EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are avail.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | Dry; ASTM D792 |
Asahi Kasei Leona® 13G43 43% Glass Filled Nylon 66 43% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Mechanical and electrical parts such as micromotors, automotive parts such as radiator tanks and shift leversInformation provi.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | |
Aremco EZ-Cast™ 580N Silicon Molding Compound Silicone Rubber Aremco's EZ-Cast™ 580N is an ideal compound for producing high reliability master molds. This silicone rubber compound exhibits high tear strength, very low shrinkage and high flexibility, all requ.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo.. |
|||
Specific Gravity | 1.50 - 1.90 g/cc | 1.50 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe UP GM 203 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant. With improved re.. |
|||
Specific Gravity | 1.50 - 1.56 g/cc | 1.50 - 1.56 g/cc | ASTM D 792 |
Karina 800-36/395-CY-RT Brown PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |