Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.48 g/cc | 1.48 g/cc | 23/23°C; ASTM D792 |
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC AMC™ 8592 is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat .. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
PolyOne Geon™ 81510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R1700L Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ISO 1183A |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
Kolon KOCETAL® TC702 Mineral Reinforced Acetal Resin Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
Kolon SPESIN® KP213G20WBL Glass Fiber Reinforced & Weather Resistant PBT Compound Resin G/F 20% reinforced, weather resistanceApplications: Parts of electric lightInformation provided by API-Kolon. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1100-7721/WT9016 Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2312EPR PEI 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 4211 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM JD4901 PEI (Asia Pacific) |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF008S PA 66 LNP* THERMOCOMP* RF008S is a compound based on Nylon 6/6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4300 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 4300 is a blue color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 4.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White P80754PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80754PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and m.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4300 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 4300 is a blue color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 4.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White P80754PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80754PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and m.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White P8550 C Concentrate Based In Polypropylene DescriptionPOLYBATCH® P8550 C is a white masterbatch containing 50% TiO2 based in homopolymer polypropylene. This product is stearate free and has been designed to offer good dispersion and excell.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | |
Dow Corning Z-1229 TETRACHLOROSILANE Fiber optic gradeInformation provided by Dow Corning |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa.. |
|||
Specific Gravity | 1.48 - 1.52 g/cc | 1.48 - 1.52 g/cc | ASTM D-792 |
Axiall 22871 Coax & Telecom Flexible PVC Non-lead, category 5 flexible CMR jacket over HDPE inners.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/10/BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
E-Polymers SEPAZ® K130IM 30% Glass Fiber Reinforced Impact Modified PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |