Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R7542X Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Specific Gravity | 1.46 - 1.52 g/cc | 1.46 - 1.52 g/cc | ASTM D 792 |
Karina E 813-10/164-B-RT-PO White PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Lanxess Durethan® BKV 40H2.0 EF 900116 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
Sylvin Technologies 8999-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
Silberline 4-Allâ„¢ E 3064AR The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
Silberline Sparkle Silver® 5271-AR Sparkle Silver® 5271-AR is medium, non-leafing aluminum pigment. It is distinguished by a closely controlled particle size distribution. This results in a fine, white, face tone with silvery pati.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
Silberline Sparkle Silver® 7005-AR Sparkle Silver® 7005-AR is a high quality, non-leafing, superfine pigment with exceptional whiteness and good flop effect. It is used mainly for its high hiding power (opacity) and distinctivenes.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
Silberline Sparkle Silver® 5500 Sparkle Silver® 5500 is a fine, regular purity, non-leafing aluminum pigment. It is characterized by a relatively wide particle size distribution.Applications: Automotive; General Industrial |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
Teknor Apex APEX® 03-A0673C-85 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS CompliantFeatures: Low Temperature Flexibility Uses: Wire Jacketing; Wire and Cable Applications Agency Ratings: UL 719Forms: Pellets Wire Types: NMB; NMProcessing Method.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SRF 1707 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.46 g/cc @Temperature 23.0 °C |
1.46 g/cc @Temperature 73.4 °F |
ASTM D792 |
DuPont Performance Polymers VESPEL TP-8556 Polyimide Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Perform.. |
|||
Specific Gravity | 1.46 - 1.50 g/cc | 1.46 - 1.50 g/cc | ASTM D-792 |
Axiall 22951 Coax & Telecom Flexible PVC Non-lead stabilized, 75C rated jacket compound suitable for riser constructions over HDPE.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
Aremco Ceramacoat™ 845-SIL High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, matte silver coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable JG552NP Polyvinyl Chloride Alloy (PVC Alloy) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |