Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion 87850 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Quadrant EPP Ketron® CM HPV PEEK Polyetheretherketone; PTFE, Graphite, and Carbon Fiber Filled Bearing Grade, compression molded (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® 3413HF PC 30% glass reinforced, high flow PC. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ AT-000/5T-2S Acetal-Copolymer, PTFE/Silicone Lubricated
(discontinued **) Description/Features:PTFE/Silicone LubricatedInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled
(discontinued **) AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Specific Gravity | 1.44 - 1.46 g/cc | 1.44 - 1.46 g/cc | |
Michelman® HydroGrease White™ 22 White coating Description: High performance water and grease resistant white coatingUsage: HydroGrease White™ 22 is a white coating which imparts water and grease resistance to the substrate. This coating is.. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 854-35/1-A-ERYB Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7781/BK PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Gromax PBT 2000-201D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | |
Sylvin Technologies 9960-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem LTX921A PEI Blend Post-industrial recycle based, 20% glass fiber filled, high flow Polyetherimide blend. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East) 20% GF Super High Flow PBT |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D794 |
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material Meldin 1357 offers the lowest wear rate and coefficient of friction, which makes it the best candidate for tribological applications. In addition, its self-lubricating properties allow it to operat.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Teknor Apex APEX® RE 8003 Polyvinyl Chloride, Rigid Features: High Impact Resistance; Medium Gloss Processing Method: Extrusion Forms: Pellets Additional Information: Performance Characteristics: Yellow Card, Interior, Medium Gloss, Excellent FinishI.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DEL359EF PC LNP* STAT-KON* DEL359EF is a compound based on Polycarbonate containing 25% Carbon Fiber, 15% PTFE. Added features include: Flame Retardant. Electrically Conductive, Wear Resistant. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | Part B |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SIH 5569 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: A; B; YI4; YI5 Agency Ratings: IEC 60502; VDE 0207 Forms: Pellets Processing .. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Light Grey 80426U Concentrate Based In LLDPE DescriptionPOLYBATCH® 80426U is a grey color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability in.. |
|||
Specific Gravity | 1.44 g/cc @Temperature 25.0 °C |
1.44 g/cc @Temperature 77.0 °F |
|
Dow Corning MOLYKOTE® 3451 CHEMICAL RESISTANT BEARING GREASE Fluorosilicone grease thickened with PTFEInformation provided by Dow Corning |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Adell DR-16 30% Glass Reinforced Polycarbonate |