Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® HydroGrease White™ 22 White coating

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name HydroGrease White™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® HydroGrease White™ 22 White coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High performance water and grease resistant white coatingUsage: HydroGrease White™ 22 is a white coating which imparts water and grease resistance to the substrate. This coating is hot melt and cold set gluable.Application data: HydroGrease White™ 22 is best applied by rod coater at the wet end of the corrugator.Food Contact Information when manufactured in the USA:FDA: 176.170: Components of paper and paperboard in contact with aqueous and fatty foods(Restricted) 176.180: Components of paper and paperboard in contact with dry foods. (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.46 g/cc
1.44 - 1.46 g/cc
pH 8.0 - 9.5
8.0 - 9.5
Brookfield Viscosity 400 - 800 cP
400 - 800 cP
Spindle # 3, rpm 60
Viscosity Measurement 16 - 22
16 - 22
[sec], EZ cup, Cup # 3
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Appearance White, opaque liquid
Solids Type Polymer/Pigment