Sylvin Technologies 9960-80 Natural PVC Molding Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sylvin Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 9960-80 Natural PVC Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
10 seconds
Tensile Strength, Ultimate 14.5 MPa
2100 psi
Elongation at Break 350 %
350 %
Tear Strength Test 320
320
Processing Properties Metric English Comments
Melt Temperature 166 - 177 °C
330 - 350 °F