Teknor Apex APEX® RE 8003 Polyvinyl Chloride, Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, High Impact , PVC, Rigid Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® RE 8003 Polyvinyl Chloride, Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: High Impact Resistance; Medium Gloss Processing Method: Extrusion Forms: Pellets Additional Information: Performance Characteristics: Yellow Card, Interior, Medium Gloss, Excellent FinishInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
10 seconds; ASTM D2240
Tensile Strength at Break 44.9 MPa
6510 psi
ASTM D638
Tensile Strength, Yield 45.0 MPa
6520 psi
ASTM D638
Elongation at Break 54 %
54 %
ASTM D638
Elongation at Yield 3.1 %
3.1 %
ASTM D638
Tensile Modulus 2.38 GPa
345 ksi
ASTM D638
Flexural Modulus 2.68 GPa
389 ksi
ASTM D790
Izod Impact, Notched 7.47 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
14.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
Compression Molded; ASTM D256
Dart Drop Total Energy 103 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.192 ft-lb/mil

@Thickness 0.125 in,
Temperature 73.0 °F
Procedure B, 0.250" Conical Dart; ASTM D4226
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 69.4 °C

@Thickness 3.17 mm
157 °F

@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 5VA
5VA
V-0

@Thickness 22.9 mm
V-0

@Thickness 0.900 in
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: